BRICS Regions to Boost Global Powder Coatings Demand

The global powder coatings demand was 1,680 kilotons in 2011 and is expected to reach 2,667.6 kilotons in 2018, growing at a compound annual growth rate (CAGR) of 6.8% from 2012 to 2018, according to a new market report published by Transparency Market Research. In terms of revenue, the market was valued at $6.5 billion in 2011 and is expected to reach $10.5 billion in 2018, growing at a CAGR of 7.2% from 2012 to 2018. The developing economies of BRICS members have led to an increasing demand for consumer goods such as appliances, automobiles and furniture. In addition, support for the use of powder coatings by authorized environmental agencies such as the U.S. Environmental Protection Agency (EPA) is another major factor responsible for the growing demand for powder coatings.

However, powder coatings do pose a few application and design difficulties, such as application of very thin coats, thin films inside corners and uneven coating thickness at edges. In addition, pigmented powders cannot be blended to form different colors. These factors are expected to hamper the growth of the powder coatings market over the forecast period.

Appliances were the largest application segment for powder coatings, accounting for over 20% of the consumption in 2011. Powder coatings demand from automotives is expected to grow at a CAGR of more than 7% during the next five years due to the rising demand of automobiles, both in terms of original equipment and spare parts across the world.

The Asia-Pacific region is the largest and fastest growing market for powder coatings, consuming over 700 kilotons of powder in 2011. Emerging end user industries in economies such as Brazil and South Africa are expected to further add to the demand for powder coatings.

For additional information, visit www.transparencymarketresearch.com/powder-coatings-market.html.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI march 2015 cover

2015 March

Welcome to our annual Raw Materials, Chemicals, Polymers and Additives Handbook!
Table Of Contents Subscribe

Paid Leave

President Obama recently announced he wants U.S. businesses and the federal government to provide paid sick leave and paid parental leave to all workers. Do you think this is a good idea?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.