WELD-ON®45 structural adhesive has received approval for Underwriters Laboratories
(UL) specification 746C. The UL certification is for use on aluminum
and for fiberglass composite substrates.
WELD-ON is a high-viscosity,
two-part methacrylate adhesive that bonds to unprepared corrosion-resistant
metals and to plastics used in sign making and plastic assembly applications.
WELD-ON is used for replacing
mechanical fasteners, rivets and welds during sign fabrication and other
component fabrication. The adhesive offers high-strength properties,
corrosion resistance and improved aesthetics, which can combine to lower
production costs.
Production advantages of WELD-ON
45 adhesives include low odor, five-minute open times, 15-minute handling
strength, high bond strength and a 12-month shelf life. The product
is available in 50ml or 400ml dual-component cartridges.
For more information, visitwww.ipscorp.com.