Krylon®Industrial Multi-Purpose Epoxy is ideal for use over prepared steel and masonry surfaces in a variety of industrial applications. This high-performance product works well with structural steel, fabrication and new construction, and features a formulation that can withstand the harsh maintenance demands of immersion environments.
Providing exceptional performance in highly corrosive environments, Krylon Industrial Multi-Purpose Epoxy can be applied at temperatures as low as 0°F, and is available in white, buff, and haze gray.
For more information, visitgo.kpgind.info/pr.