ASI Magazine
  Home
  ASI Green
  Subscribe
  eNewsletter Subscription
  Subscription Customer Service
  Updates
  Calendar of Events
  Call for Papers
  Features
  Columns
  Today's Headlines
  Price Adjustments
  New Products
  Ad Index
  Podcasts
  Ask Dr. Dave
  ASI Blog
  Online Exclusives
  Adhesives in the News
  Resources
  Books
  Archives
  Digital Edition Archives
  Classified Ads
  Career Center
  Tech ManufactureXPO
  Industry Links
  Online Solutions Web Seminars
  This to That
  Services Marketplace
  E-Newsletter Archives
  Green Opportunities E-News Archives
  Market Research
  Literature Showcases
  Glossaries
  Directories
  ASI Info
  Media Kit
  Contact Us
  Sales Staff
  Reprints
  List Rental
Search in: EditorialProductsCompanies
Ask Dr. Dave
by Dr. Dave Dunn
July 1, 2008

ARTICLE TOOLS
EmailEmailPrintPrintReprintsReprintsshareShare



Question: I typically deal with both epoxy and acrylic systems. Do you have any tips for making my adhesives fire retardant?

Answer: Fire retardants have historically been based on either inorganic materials or halogenated organic compounds. The entire subject of fire retardancy has been hotly debated in recent years because of the negative environmental aspects concerned with certain brominated materials. Phosphate and phosphonate compounds are typical alternative flame-retardants that do not make use of halogens. In adhesives, the choice of fire retardants is dependent on the type of system you are using. In a typical filled epoxy system, you can almost certainly use a combination of a solid inorganic fire retardant such as aluminum trihydate or magnesium hydroxide, perhaps supplemented by an organic one. However, if you have an unfilled acrylic system, particularly one with low viscosity, the choice of materials is much more limited. In this case, you might consider the handful of brominated or phosphorous-containing monomers that can be co-polymerized into the adhesive. There are several suppliers who specialize in fire retardants, and they can advise you on both product performance and safety aspects.



Question: What sort of approvals do I need for sealants used on pipes carrying potable water?

Answer: Sealants for contact with drinking water must be certified to a national standard called ANSI/NSF Standard 61. Several organizations are accredited by ANSI (American National Standards Institute) to test and certify this sort of product. The testing involves exposing the cured sealant to standardized test waters at specified temperatures and times and analyzing the extraction water for target contaminants. Results of this laboratory testing are then “normalized” to estimate their concentrations in specific pipe sizes or tanks, and a material will normally be certified for specific sizes and for specific water temperature use, defined as commercial hot water (180°F), “domestic” hot water (140°F), or cold water. The entire process of obtaining this certification can take many months, and I would advise reading the standard carefully before initiating testing so that you know the target contaminants and can determine whether or not your sealant has a good chance of passing the extraction testing.


Dr. Dave Dunn
DrDave242@windstream.net
Q&A Exchange is written by Dr. Dave Dunn of F.L.D.Enterprises, a technical consultancy and full-service industrial market-research firm specializing in the adhesives, sealants, specialty rubbers and plastics fields. Dr. Dave is a former vice president and director of Loctite Corp. and has spent many years in troubleshooting adhesive and sealant problems. Questions for publication should be directed to him at 242 Trails End, Aurora OH 44202; phone 330-562-2930; fax (330) 247-1690; e-mail DrDave242@windstream.net .

Links

|PrintEmail

Did you enjoy this article? Click here to subscribe to the magazine.







© 2010 BNP Media. All rights reserved. The publisher is not responsible for product claims and representations. Any views or opinions expressed are those of the author and do not represent those of ASI magazine, its staff, Editorial Advisory Board or BNP Media. | Privacy Policy