A new family of acrylic tape products is now available for low-surface-energy (LSE) materials used in the automotive, medical device, electronics and transportation markets. The 650 tape systems have reportedly been expanded and engineered specifically for high-performance, durable-bonding LSE applications and are available in double-sided PET, double-coated tissue, and an array of unsupported transfer tape products with application-specific poly-coated, board or film release liners.
The tapes are suitable for a variety of open and closed-cell foams, low-surface-energy substrates such as TPOs, and powder-coated paint surfaces.