Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEW PRODUCTS
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • EVENTS
    • ASI Academy
    • Events Calendar
  • COLUMNS
    • European Perspectives
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Classifieds
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
      • Custom Content & Marketing Services
    • CONTACT
  • SIGN UP!
Finished Adhesives and SealantsPressure-Sensitive Adhesives (PSAs)FormulatorsManufacturers

The Quick Fix: A Brief, Early History of Tape

By Tisha Hooks
January 4, 2013

There is no patent for duct tape. Yet objects do not simply appear out of nowhere. They have histories and their histories have histories. The stories of how they came to be are just as important and arguably as deeply influential as their use. For objects are never simply objects. They are ideas and aspirations, solutions, frustrations, symbols, and placeholders. Though many pressure-sensitive tapes have been created with durability in mind, there is a way in which we understand tape as the expedient, quick fix.

Rubber

Although adhesives have been around for centuries in one form or another, tape’s story stretches back to at least the 1700s with the “discovery” by the West of rubber and rubber-based adhesives. In 1736, when Charles Marie de la Condamine of France returned home from the New World bearing latex—the milky substance extracted from rubber plants—he set out on a cycle of experimentation and invention that would lead to exponential scientific innovation. By the mid-18th century, improvements in processing such as vulcanization, in which rubber is treated with high heat and sulfur and made more durable, led to the development of everything from waterproof raincoats and revolver hand grips to electric insulation and beauty products.1

Cotton

After the Civil War, when sharecropping, tenancy, and itinerant labor replaced the slave-based plantation economy for the Southern poor, cotton continued to fuel the U.S. economic engine. For well over a century, from 1803-1937, cotton remained the nation’s leading export.2

Eli Whitney’s cotton gin went into production in 1794. The difference in the percentage of the European textile market held by cotton prior to and after its invention was profound, from 6% in the 1780s to 77% in the 1880s3 (see Figure 1).

Medicinal/First Aid Applications

Relatively inexpensive rubber and cotton realized greater innovation in other industries, including those involving pressure-sensitive adhesives. In 1845, William Harral Shecut and Horace Day received an early patent for Improvement in Adhesive Plasters.4 They combined “cotton cambric or muslin” with India rubber that had been boiled, covered in turpentine, and mixed with cayenne pepper, ground litharge, and melted pine-gum.

The innovation didn’t end with the processing of the rubber, however. The penultimate product was perforated to allow the skin underneath to breathe when applied.5 After the Civil War, medical product manufacturers like Seabury & Johnson and later Johnson & Johnson had their first significant successes with medicinal plasters. An 1893 Johnson & Johnson publication noted that the employment of India rubber in plasters was “the first progressive step in plaster making…in centuries of pharmacy.” What distinguished India rubber was that it was “just the right stickiness at body temperature,” reacted favorably with nearly all medications, and was “waterproof” and “stable,” although to be sure, it remained “a highly complex and treacherous substance.”6

The rise of companies like Johnson & Johnson was the result of not only scientific and technological innovation, but also a late 19th-century concern for cleanliness and public hygiene, the call for increasing standardization and accountability, and greater professionalization in medicine and the pharmaceutical industries that supplied it. In addition, with the founding of the Red Cross in 1881 came a greater emphasis on providing basic medical training and supplies for civilians. Soon, companies were creating first-aid kits for railroad workers, factory workers and sports teams.

In 1920, Earle Dickson, a cotton buyer for Johnson & Johnson, invented what would become the Band-Aid® to meet the needs of his wife, who often nicked herself with a kitchen knife when preparing meals. A pressure-sensitive tape with a cotton layer and a waterproof backing, the Band-Aid became a staple of the first-aid kit.7

Home/Industrial Use

By the turn of the 20th century, manufacturers of surgical tape—be it Johnson & Johnson’s Zonas® Adhesive Plaster8 or Bauer & Black’s Adhesive Plaster Tape—had recognized a market beyond the medicinal. As shown in Figure 2, Bauer & Black touted their product as the “everyday first-aid,” suitable for fixing everything from plumbing, to abraded hands and feet.”9

In 1923, while making deliveries for 3M, Richard Drew happened on one of the more unusual deployments of surgical tape—mapping out the edges of car paint jobs—and decided he could come up with something far less expensive. After much experimentation, he applied a layer of adhesive to a thin paper, and both masking tape and 3M as producers of tape were born.10

During World War II, companies such as 3M and Johnson & Johnson would produce industrial tapes like duct tape for packaging material in order to limit the corrosive effects of the environment on bullets and metal parts sent overseas. Given tape’s links to medicine and first aid, its ease of use, and flexibility, as well as its history of preservation, little wonder that in 2003 it would be called upon to hold together an anxious nation by the U.S. Department of Homeland Security.
Technologies have histories, and their histories have histories.


For more information, contact the author at tisha.hooks@yale.edu.

Author’s acknowledgement: Special thanks to John Johnston and Jerry M. Serra for sharing their invaluable expertise.

Editor’s note: This article is based on a poster presentation given at the Pressure Sensitive Tape Council’s Tech 35 in Boston.

References
1. Tully, John, The Devil’s Milk: A Social History of Rubber, Monthly Review Press, 2011, 32.
2. Dattel, Eugene R., Cotton and Race in the Making of America: The Human Costs of Economic Power, Chicago: Ivan R. Dee, 2009, 35.
3. Ibid., 49.
4. Satas, Donatas, ed., Handbook of Pressure-Sensitive Adhesive Technology, New York: Van Nostrand Reinhold, 1982, 3.
5. Shecut, William H., and Day, Horace H., Improvement in Adhesive Plasters, U.S. Patent 3,965, March 26, 1845.
6. Kilmer, F.B., ed., Belladonna: A Study of Its History, Action, and Uses in Medicine, New York, NY: Johnson & Johnson, 1893, 35.
7. “BAND-AID® Brand Adhesive Bandages Beginnings,” Johnson & Johnson Consumer Companies, Inc., Band-Aid.com, 2011 and 2007, www.band-aid.com/brand-heritage.
8. Gurowitz, Margaret, “ZONAS®—The Duct Tape of Its Day,” Kilmer House: The Story of Johnson & Johnson and Its People, September 9, 2009, www.kilmerhouse.com/2009/09/zonas-the-duct-tape-of-its-day/.
9. Bauer & Black, “Adhesive Plaster Tape: The Everyday First Aid Advertisement,” The Red Cross Magazine, August 1918.
10. Feyder, Susan, “Scotch Brand Tape—a ‘Free Spirit’s Invention,’” St. Paul Sunday Pioneer Press—Business, St. Paul, MN, October 5, 1975.

KEYWORDS: bonding films tapes

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Tisha Hooks is a Ph.D. Candidate at Yale University.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • linked network nodes

    Using the Power of AI for Adhesive and Sealant Formulation

    With the help of software solutions, adhesive formulators...
    Adhesives and Sealants Topics
    By: Karen Parker
  • ASI top 20 global manufacturers

    2025 ASI Top 20: Leading Global Adhesives and Sealants Manufacturers

    ASI's annual ranking of the top 20 global adhesive and...
    Pressure-Sensitive Adhesives (PSAs)
    By: Karen Parker
  • science test tubes

    2026 Adhesives and Sealants Raw Materials Roundup

    After more than two years of contraction, the...
    Sustainability
    By: Karen Parker
Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

Image of a blue bar chart with arrow pointing up

Iran War and Logistics Challenges Impact Adhesives and Sealants Pricing

news on internet screen

H.B. Fuller and Ancora Holdings Clash Over Proposed Medical Adhesives Acquisition

Aerial picture of a chemical facility

DELO Reports Record Revenue for Fiscal Year

ASI Top 20 website

Events

June 15, 2026

Adhesive and Sealant Council Executive Leadership Conference

This annual event provides current and future leaders in the adhesives and sealants industry with the opportunity to expand their knowledge and network with peers.

September 14, 2026

Women in Chemicals Conference

Organized by Women in Chemicals, this landmark conference will offer opportunities for networking, learning, and professional development. With a diverse array of sessions, workshops, and social events, participants can expect a dynamic program designed to empower and inspire.

View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

ASI CASE EBOOK

ASI raw materials roundup

Related Articles

  • digital graphic representing a connected world

    3M Continues History of Innovating for The Future

    See More
  • from the editor

    Neanderthal 'Factory' and the Long History of Innovation

    See More
  • History Channel Presents History of Glue

    See More

Related Products

See More Products
  • Optimizing Social Media from a B2B Perspective

  • Handbook of Adhesives and Surface Preparation

  • Handbook of Sealant Technology

See More Products

Related Directories

  • The Griff Network

    The Griff Network is an ISO 9001:2015 certified manufacturer of papers, films, laminates, and membranes for the industry. We specialize in roll and sheet converting, lamination, release and adhesive coating, product development, and more! Visit us online for more information. Call us for a quick quote.
×

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing