Here’s an example of sealants going to the birds, literally.




Here’s an example of sealants going to the birds, literally: BioBased Systems®, a polyurethane spray foam custom manufacturer, worked in conjunction with agricultural insulation experts to manufacture a line of soy-based insulations and sealants specifically for agricultural uses. The products help growers combat the difficulty that many poultry farmers are having with affording the propane to heat their chicken houses.

BioBased Systems manufactures custom spray-foam products that integrate soy ingredients, namely Agrol® polyols, to replace petroleum ingredients typically found in traditional spray polyurethane insulations and sealants. The agricultural insulation and sealant products are all water blown (versus HCFC blown) and are applied directly to the walls of the chicken house. This means the product won’t sag or settle over time, like some conventional insulations. When the insulation or sealant is sprayed onto a wall, footer, or roof deck it expands and fills all of the cracks, crevices and voids. As an inert thermo-set plastic, these products are extremely durable.

A study conducted by Auburn University in conjunction with Ag-Tite, a BioBased Systems client, indicated that an analysis of data on poultry houses treated with a soy sealant for one year showed a savings of 35% in energy costs compared to a traditional insulation treatment. Annual heating and fuel savings were 1,850 gallons per poultry house after the treatment.

"We see that in almost all cases, payback of the initial energy retrofit cost is within three years," says Josh Hutchinson, Agricultural Systems Manager for BioBased Systems. Soy-based foam insulation and sealant treatments are not only energy efficient, but they act as a barrier to irritants like mold and pollen.

Sealing up the house creates a more comfortable environment for the chickens to grow in, meaning that they become bigger, healthier and more tasty birds: a win-win for both the adhesives and sealants industry and carnivores everywhere.

The soybean checkoff supported the development and growth of the soy-based spray polyurethane foam category, which has already grown quite large in the residential and commercial construction market. It appears that the agricultural market is showing similar promise as a new use for soy.

For more information, www.ag-title or www.agseal.com.

To learn more about new uses for soy, visit www.soynewuses.org.


You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40