Blade Bonding
May 1, 2010
 |
| ATBV25 wind turbine. |
|
Improved
bonding methods for wind turbine blade production and blade servicing.
 |
| Vacuum-infusion process. |
|
The use of wind energy is expected to grow at an
unprecedented rate. Developments in wind energy are presenting new challenges
to designers and engineers. For example, with a demand for increase in wind
turbine blade size comes an exponential increase in the performance
requirements of the materials used. Research continues in the use of structural
adhesives to bond composite wind turbine components. ITW Plexus is a leader in
this field, and its work is benefitting a number of manufacturers.
Turbine blades are traditionally bonded with relatively slow-curing epoxy
systems, polyesters and two-part polyurethane adhesives. ITW Plexus has
developed long-working-time, fast-curing, 1:1 methacrylate structural adhesives
that produce bonds that hold after the substrates delaminate. Unlike
traditional adhesives, these advanced methacrylate adhesives chemically fuse
FRP/GRP, composite stiffener spars and perimeter flange joints. They also
provide increased peel resistance and cycle fatigue resistance while reducing
damage during transportation. Room-temperature snap-cure properties have helped
to increase production rates and eliminate the expenses and energy costs
associated with post curing, which is required to cure some epoxies. What’s
more, little or no surface preparation is required.
The company’s MA560 and MA590 adhesives have gained acceptance in this growing
marketplace because they also increase blade performance and reduce processing
time.
Design Requirements for Turbine Components and Adhesives
 |
| Figure. Shear Strength Comparisons of Plexus Products |
|
Three main factors must be considered for construction of
turbine components.
1. Effective Bending and Fatigue Resistance
Effective bending and fatigue resistance is a major consideration in blade
design — the outer composite shell cannot perform this function without the
assistance of internal stiffening. Box and C-shaped structures are often used
to provide the required bending strength and stiffness (see Figure); these
stiffening structures are bonded to the interior of the turbine blade.
2. Strength and Durability
Since the blade parts are generally bonded together, strength and durability of
the adhesive bonds are major design factors. These can become limiting
performance factors in conjunction with the performance of the composite
itself.
According to blade qualification procedures, the bending strength and fatigue
strength of a blade must be sufficient for a 20-year life. In addition, part of
the procedure requires full-scale testing on prototype blades.
 |
| ATBV25 wind turbine fiberglass blade. |
|
3. Adhesive Requirements
Several requirements are necessary for adhesive bonds for wind turbine blades.
- Adhesives must withstand the centrifugal forces applied to each
blade.
- High stress, fatigue and aging resistance is
required.
- To ensure long-lasting joints, the adhesive must withstand outdoor
exposure, significant temperature ranges and lap shear strengths in the range
4,000 psi (27 MPa).
- Adhesives must maintain the bond strength for the blade’s lifetime,
as they are used to bond two halves of a blade and the spar while filling
substantial gaps on structures up to 60 meters long.
- Bonds must endure lifetime ambient conditions with daily cycling.
- Improved cure profiles and reduced peak temperatures are required.
The new adhesives developed by ITW Plexus for the wind sector offer the
following attributes.
- Composites are chemically fused to give strong bonds.
- Adhesives require little or no surface preparation and provide high
resistance to stress, fatigue, and outdoor exposure.
- Products contain a room-temperature curing mechanism.
- Certification by Germanischer Lloyd Wind Energy (GL Wind).
By using these products, manufacturers can enjoy the following benefits:
- Reduced production costs.
- Shortened assembly times.
- Increased throughput.
- Reduced component weight.
- Improved blade quality and manufacturing process.
- Excellent water and UV resistance.
- Competitive performance, cost effectiveness and reliability.
Field Servicing of the Blades
 |
| Internal section of a wind blade, showing the bonding lines of the blade parts and spar. |
|
ITW
Plexus' adhesives/fillers are becoming a standard for servicing wind blades in
the field. Plexus MA530 and MA425 adhesives can fill gaps up to 18 mm in depth
and are now being used to fill cavities. Because of their good adhesion, these
products are less dependent on surface condition. In addition, the adhesives do
not require heat for curing, which gives service engineers the flexibility to
do work in the field.
About the Company
ITW
Plexus is a division of Illinois Tool Works (ITW) Performance Polymers Europe
(ITWPPE). ITW is a diversified industrial company with 2008 sales of $16
billion. Established in 1912, the company employs 60,000 people worldwide. The
Performance Polymers Europe division has more than 25 years of experience in
the design, development and production of UV-curing, epoxy, and methacrylate
bonding agents. Its ongoing adhesive R&D program is based at its UK and
German laboratory facilities.
For more information, phone (870) 458-7588 or visit www.itwplexus.eu.
SIDEBAR: Case Study: Terom Wind Energy, Bologna, Italy
Terom Wind Energy has designed and manufactured the ATBV26,
a small wind turbine suitable for low-wind-speed sites. The turbine uses a
wide-diameter rotor and technology that involves a multi-pole direct drive
permanent magnet generator, variable pitch, active pitch and yaw control
system. Nominal power is reached at a wind speed below 8 m/s, and energy yield
is particularly high: 3,000 equivalent hour production in a site with average
wind speed of 5 m/s.
Glass fiber-reinforced polymer blades have been internally designed and are
produced using a vacuum-infusion process. This system allows complete
saturation of glass reinforcements with resin and offers a good fiber-to-resin
ratio, since the vacuum minimizes air pockets forming between fibers and the
permeability of the fiberglass. Blade components, made using special molds, are
then finished and bonded together using a Plexus structural adhesive. The
result is a strong but lightweight product with good mechanical-resistance
properties.
|