CASS POLYMERS: Epoxy Paste
ADTECH Plastic Systems' Edge Seal 2017 is a low-density, flame retardant, two-part epoxy material that does not contain polybrominated diphenyl ether (PBDE) or other brominated flame retardant components. The smooth, creamy consistency is ideal as an edge sealant for honeycomb core structures. Edge Seal 2017 is color-coded to ensure proper mixing, cures to a charcoal gray color, and - when used at room temperature - can be sanded in 4-6 hours. Edge Seal 2017 was developed to meet BMS 5-28 Type 17 and FAR/JAR 25.853(a).