ASI Magazine
  Home
  ASI Green
  Subscribe
  eNewsletter Subscription
  Subscription Customer Service
  Updates
  Calendar of Events
  Call for Papers
  Features
  Columns
  Today's Headlines
  Price Adjustments
  New Products
  Ad Index
  Podcasts
  Ask Dr. Dave
  ASI Blog
  Online Exclusives
  Adhesives in the News
  Resources
  Books
  Archives
  Digital Edition Archives
  Classified Ads
  Career Center
  Tech ManufactureXPO
  Industry Links
  Online Solutions Web Seminars
  This to That
  Services Marketplace
  E-Newsletter Archives
  Green Opportunities E-News Archives
  Market Research
  Literature Showcases
  Glossaries
  Directories
  ASI Info
  Media Kit
  Contact Us
  Sales Staff
  Reprints
  List Rental
Search in: EditorialProductsCompanies
New "Electronic Glue” Promises Less-Expensive Semiconductors

October 1, 2009

ARTICLE TOOLS
EmailEmailPrintPrintReprintsReprintsshareShare

A vial of nanocrystals in solution, which serve as “electronic glue” for semiconductor-based technologies.


University of Chicago Postdoctoral Scholar Maksym Kovalenko (left) working with nanocrystals in a glovebox in the laboratory of Dmitri Talapin, assistant professor in Chemistry. Working in the environmentally controlled conditions of the glovebox permits researchers to perform chemical procedures not possible under room conditions.

Photos by Dan Dry.
Researchers at the University of Chicago and Lawrence Berkeley National Laboratory have developed an “electronic glue” that could accelerate advances in semiconductor-based technologies, including solar cells and thermoelectric devices that convert sunlight and waste heat, respectively, into useful electrical energy.

Semiconductors have served as choice materials for many electronic and optical devices because of their physical properties. Commercial solar cells, computer chips and other semiconductor technologies typically use large semiconductor crystals, but these are expensive and can make large-scale applications such as rooftop solar-energy collectors prohibitive.


Dmitri Talapin is an assistant professor in Chemistry at the University of Chicago.
As an alternative, engineers see great potential in semiconductor nanocrystals that sometimes measure just a few hundred atoms each. Nanocrystals can be readily mass-produced and used for device manufacturing via inkjet printing and other solution-based processes. But a problem remains: The crystals are unable to efficiently transfer their electric charges to one another due to surface ligands — bulky, insulating organic molecules that cap nanocrystals.

The “electronic glue” developed in Dmitri Talapin’s laboratory at the University of Chicago solves the ligand problem. The team describes in the journal Science how substituting the insulating organic molecules with novel inorganic molecules dramatically increases the electronic coupling between nanocrystals. The University of Chicago licensed the underlying technology for thermoelectric applications to Evident Technologies in February.


Sources

Citation: “Colloidal Nanocrystals with Molecular Metal Chalcogenide Surface Ligands,” Maksym V. Kovalendo, Department of Chemistry, University of Chicago; Marcus Scheele, Molecular Foundry, Lawrence Berkeley National Laboratory; and Dmitri V. Talapin, Department of Chemistry, University of Chicago, and Center for Nanoscale Materials, Argonne National Laboratory, Science, June 12, 2009.

Funding sources: American Chemical Society Petroleum Research Fund, The Chicago Energy Initiative, U.S. Department of Energy and Evident Technologies Inc.