Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEW PRODUCTS
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • EVENTS
    • ASI Academy
    • Events Calendar
  • COLUMNS
    • European Perspectives
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Classifieds
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
      • Custom Content & Marketing Services
    • CONTACT
  • SIGN UP!

Natural-Based Adhesives for Packaging and Converting

November 1, 2004
From stone age technology to what's new

Photo by Lindsay Thompson

Casein can be formulated to make cold water resistant, ice-proof bottle labeling adhesives, which, when properly formulated, can be removed in an alkaline soaker.



Although other adhesive technologies and forms, such as hot melts, have taken some market share in recent years, natural-based waterborne adhesives are still very popular, are growing in volume and will be used for many years to come. They are the adhesives of choice in many industries.

This article will focus on the use of starch- and casein-based adhesives for labeling, and the use of dextrin-based adhesives in the envelope market.

Natural Adhesives for P&C Applications

Contrary to popular belief, hot melts do not dominate the packaging and converting (P&C) industries. All available information points to P&C adhesives being primarily waterborne and suggests that a sizable percentage of these adhesives are natural based.

Following are some statistics.

  • U.S. formulated adhesive industry - P&C 47%, waterborne 58.9%.1
  • Natural-based adhesives, from a global standpoint, comprise about 37% of the total demand.2
  • Starch and dextrin adhesives account for approximately 58% of the U.S. packaging market.3

Seeing these figures, one has to wonder if flexible packaging, corrugated starches, etc., are included. At any rate, there is no doubt that P&C is a large adhesive market and that natural-based adhesives are an important part of that market - although frequently ignored.

Waterborne adhesives are certainly a mature technology. However, the market is very large and one can sell adhesives to many of the P&C adhesive markets as specialty products. In addition, some of the newest adhesive developments, such as reactive hot melts, 100%-solids flexible packaging adhesives, and low-temperature-application hot melts, have been funded by the sales profits of waterborne adhesives. This will continue in the years ahead.

Waterborne adhesives and natural-based products are alive and well. They continue to grow in use, although at a slower rate than hot melts.

This article will concentrate on the P&C markets, waterborne adhesives, and natural-based waterborne adhesives.

Types of Natural-Based Adhesives

The major natural-based waterborne adhesives used for P&C are those based upon starch, dextrin, and casein. Major markets for these products include the following.
  • Starch - labeling (jelly gum), envelope, bags and sacks, bookbinding, tissue and towels, cigarettes
  • Dextrin - general packaging, labeling, case and carton sealing and forming, envelopes and gumming, bags and sacks, tube and core winding, tissue and towels, laminating, cigarette packaging
  • Casein - labeling

Starch-Based Adhesives

Starches used in the U.S. adhesives industry are primarily those based on maize (corn), waxy maize, tapioca and potato. Corn-based products are most widely used. Some adhesives will have a mixture of various types of starches. Raw and acid fluidities and oxidized starches are used to make adhesives. Also see comments under the labeling section to follow.

Dextrin-Based Adhesives

Dextrins are widely used in the P&C industry. Dextrins are composed of starches converted by acid, heat or a combination of both. There are slightly converted dextrines, highly converted dextrins and ones in between.

Generally, the higher the conversion, the higher the water solubility; likewise, the higher the solids, the tackier the adhesive, but the poorer the adhesion. Dextrins can be classified by the type of conversion and the extent of the conversion - white dextrines, yellow dextrines and British gums. Where greater tack, solubility, remoistenability and clarity are desired, root dextrines (tapioca or potato) are used, such as in envelope front seals.

Borated dextrines are widely used for P&C. Borated dextrines are what the name implies - dextrin, borax, and, in most cases, sodium hydroxide. The borax increases the tack and speed, and the caustic reinforces the borax effect.

Casein-Based Adhesives

Casein-based adhesives are widely used for the labeling of glassware. An example is the large consumption of adhesives in breweries.

Casein is a dry protein obtained from cow's milk. It can be formulated to make cold water resistant, icewater-proof (IWR) bottle labeling adhesives, which, when properly formulated, can be removed in an alkaline soaker.

Markets

Glass Bottle Labeling and Envelopes

The labeling market is a very large one. It has been estimated that it represents about 6% of the packaging market.4 At least 50% of the labels used are glue applied. Some 90% of the labels used in the food and beverage markets are glue applied.4

The three main types of adhesives used for glass bottle labeling are starch-based (jelly gum), casein and non-casein. The sidebar shows a comparison of these three types of adhesives.

Starch-based jelly gums (alkaline types) are made by slurrying the starch in water, heating, and mixing with sodium hydroxide to convert the starch into a viscous mass. Acids are used to stop the conversion of the starch at the desired point. Other additives, such as deformers, preservatives and salts, are used. pH control is important.

The starch used to make jelly gums can be waxy maize, potato, tapioca, sago or a combination of these. Each starch will give slightly different properties.

Jelly gums are very tacky adhesives with good adhesion to glassware, but they do not have IWR. Jelly gums can be formulated to run well on picker and rotary labelers.

Casein is obtained from cow's milk and thus is subject to the whims of nature, the season, cost, and importation. However, casein-based IWR adhesives are excellent machining products on rotary- and picker-type labelers, and, when properly formulated, have IWR but can be removed in alkaline soakers such as those used in breweries. IWR casein adhesives contain casein, a peptizer, a crosslinker to provide IWR, ammonia, and perhaps some starch, preservatives, defoamers, etc. IWR casein-based adhesives are fast and tacky and can adhere to moist glassware. Casein-based adhesives are sometimes subject to bacterial attack.

A non-casein IWR labeling adhesive is the name given to products formulated to have IWR that still do not contain casein. They are based upon starch, special polymers and resin additives. They have very good IWR but are more difficult to remove in alkaline soakers than casein adhesives. In addition, these types of adhesives sometimes have a very strong ammonia odor.

Envelopes

Dextrines are widely used as the base for the remoistenable adhesive (called the front seal gum) used on an envelope. Front seals must have: good adhesion to a variety of paper stocks; a light color; gloss; a flat lay; the ability to dry quickly; high-humidity resistance to prevent blocking; and the ability to machine well.

The dextrines used in envelope front seals are generally root starch-based because root starch dextrines have better clarity and stability than maize-based starch dextrines. It is possible to make an envelope front seal using a combination of root and maize dextrines. "Yellow" dextrines and British gum dextrines used for envelope front seals are highly converted dextrines.

Envelope dextrin front seals are formulated from dextrin, bleaching agents, stabilizers, various types of humectants, wetting agents and preservatives. Typical dextrin front seals have a viscosity of 6000-9000 cps and a solids content of 65% or so.

In addition to the "all dextrin" front seals, there are dextrin + vinyl resin formulas (generally 10-25% or so of vinyl resin) and vinyl resin + dextrin formulas (generally 60% or so of vinyl resin).

The dextrin-compatible vinyl acetate resin emulsion provides faster drying speed, adhesion and tack when remoistened.

Trends and Opportunities

Labeling
  • Improved machining IWR casein adhesives - less splashing and slinging, even at speeds in excess of 1000 bpm
  • Non-casein IWR adhesives with improved removability in alkaline soakers
  • Growth of sleeve and wraparound roll-fed film labels using hot melts
  • UV-curable hot melts for shink labels with high shrink

Envelopes

  • Improved non-splashing, non-throwing, clean-transfer, good-adhesion and minimal penetration starch-based back seam gums
  • Good-machining window gums
  • Front seals with superior adhesion to a variety of paper stocks
  • Front seals with an optimum balance between non curl, high humidity blocking resistance, gloss, speed and cost effectiveness


Conclusion

The waterborne adhesive market is a mature market; natural-based products are generally considered mature as well. However, that does not mean that all of these types of products should be presented and sold as commodities. Adhesives are specialty products. Some industries need such specialty adhesives - products with special properties of value to the customer along with close sales and technical support. Industries where this is possible include the ones mentioned, but there are others.

This article is based on a paper presented at the Spring 2004 Adhesive and Sealant Council, Inc. meeting in Cleveland.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • linked network nodes

    Using the Power of AI for Adhesive and Sealant Formulation

    With the help of software solutions, adhesive formulators...
    Raw Materials and Chemicals
    By: Karen Parker
  • ASI top 20 global manufacturers

    2025 ASI Top 20: Leading Global Adhesives and Sealants Manufacturers

    ASI's annual ranking of the top 20 global adhesive and...
    Adhesives and Sealants Topics
    By: Karen Parker
  • science test tubes

    2026 Adhesives and Sealants Raw Materials Roundup

    After more than two years of contraction, the...
    Sustainability
    By: Karen Parker
Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

Image of a blue bar chart with arrow pointing up

Iran War and Logistics Challenges Impact Adhesives and Sealants Pricing

news on internet screen

H.B. Fuller and Ancora Holdings Clash Over Proposed Medical Adhesives Acquisition

Picture of five men standing in front of a machine

Henkel Inaugurates Modernized Packaging Competence Center

ASI Top 20 website

Events

June 15, 2026

Adhesive and Sealant Council Executive Leadership Conference

This annual event provides current and future leaders in the adhesives and sealants industry with the opportunity to expand their knowledge and network with peers.

September 14, 2026

Women in Chemicals Conference

Organized by Women in Chemicals, this landmark conference will offer opportunities for networking, learning, and professional development. With a diverse array of sessions, workshops, and social events, participants can expect a dynamic program designed to empower and inspire.

View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

ASI CASE EBOOK

ASI raw materials roundup

Related Articles

  • H.B. FULLER CO.: Laminating Adhesives for Packaging

    See More
  • CONVERTING/PACKAGING END USER: Fresh Opportunities for the Packaging Industry

    See More
  • Eco-Friendly Adhesives for Converting and Packaging

    See More

Related Products

See More Products
  • biobased wood.jpg

    Bio-based Wood Adhesives: Preparation, Characterization, and Testing

  • Pressure-Sensitive Adhesives and Applications

  • Handbook of Adhesives and Surface Preparation

See More Products

Related Directories

  • Capital Adhesives Inc.

    Since 1987, Capital Adhesives has focused on helping customers stay ahead with expert support and technical know-how. We've built a full lineup of specialty adhesives and coatings tailored for markets like printing, packaging, textiles, and converting.
×

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing