Green Microsite
  Home
  ASI Green
  Subscribe
  eNewsletter Subscription
  Subscription Customer Service
  Updates
  Calendar of Events
  Call for Papers
  Features
  Columns
  Today's Headlines
  Price Adjustments
  New Products
  Ad Index
  Podcasts
  Ask Dr. Dave
  ASI Blog
  Online Exclusives
  Adhesives in the News
  Resources
  Books
  Archives
  Digital Edition Archives
  Classified Ads
  Career Center
  Tech ManufactureXPO
  Industry Links
  Online Solutions Web Seminars
  This to That
  Services Marketplace
  E-Newsletter Archives
  Green Opportunities E-News Archives
  Market Research
  Literature Showcases
  Glossaries
  Directories
  ASI Info
  Media Kit
  Contact Us
  Sales Staff
  Reprints
  List Rental
Search in: EditorialProductsCompanies
PPG Aerospace Begins Use of Chromate-Free Moisture Seal on Windshields (6/16/09)

June 16, 2009

ARTICLE TOOLS
EmailEmailPrintPrintReprintsReprintsshareShare



PPG Industries’ aerospace business has begun using its chromate-free polysulfide aircraft window sealant on its glass-faced acrylic replacement windshields for Bombardier Challenger 600 Series business jets to provide operators with an environmentally responsible moisture seal.

It is the first commercial application for PR-1425CF sealant, according to Jim Romano, PPG Aerospace global sales director for commercial aftermarket transparencies.

The PPG glass-faced acrylic replacement windshield for Challenger 600, 601, 604 and 605 jets combines the chemical and abrasion resistance of glass with the weight-saving benefits of plastic. The new-design windshield has an expected service life of more than double that of the all-acrylic part it replaces, based on expected service life of similar windshields.

“Benefitting from its unique position as a leader in aerospace sealants and transparencies, PPG Aerospace brings PR-1425CF sealant to market with about 4,000 hours of in-flight test data on different airframe types,” Romano said.

PPG tests also have shown PR-1425CF to be compatible with PR-1425 polysulfide sealant, so the new fast-curing, environmentally responsible sealant can be used to repair a moisture seal made with PR-1425 sealant, he said.

PPG has extended its offer to qualified operators of Challenger 600 Series jets of a $10,000 rebate through the end of August on purchases of the new-design glass-faced acrylic replacement windshield, which lists for $52,000.

Paris Air Show visitors can see the new-design glass-faced windshield for Challenger 600 Series jets and get information about PR-1425CF sealant at PPG Aerospace’s display at Hall 2B, Stand D57. The International Paris Air Show is scheduled for June 15-21 at Le Bourget Exhibition Centre.

For more information, visit www.ppgaerospace.com.