Working towards greater sustainability in the packaging and labelling sectors, Beardow Adams has developed an environmentally friendly adhesive.
The new, FDA approved adhesive, BAM 2537, allows returned bottles to be washed in a caustic solution, separating them from their labels and the adhesive, before being returned to the market. This reuse loop can take place between 10 to 15 times before the bottle is fully recycled – drastically reducing the number of single-use plastics.