XLYNX Materials announces the launch of PlastiLynx PXN, an advanced PFAS-free universal primer that modifies the surfaces of hard-to-bond polyolefins to enable strong adhesion with glues, coatings, and dyes.
Low surface energy polymers like polypropylene (PP) and polyethylene (PE) are highly valued because of their lightweight strength, affordability, and resilience. However, their incompatibility with adhesives has been an obstacle for many applications. Conventional primers and surface treatments offer imperfect solutions to this problem.