A good way to detect whether a screw has been interfered with is to cover it with a unique type of encapsulant that will show whether it has been removed and is not readily available to an end user. The simplest way to do this is to add a readily detectable ingredient to the encapsulant such as an unusual color or a fluorescing material so you can detect your material under a black light.