SW200 Removable is a tape specially designed for applications where ultra-low removable pressure-sensitive adhesive is desired. This self-wound tape serves as a protective film when used as a post-mask in die-cut operations to facilitate waste removal from a substrate. The process also ensures cleaner removal of punched waste, as well as eliminates, or lessens, the need for vacuum removal of ambient dust or other airborne contaminants. The tape is available in widths up to 54". Properties include peel strength of 4-8 oz/inch of width, breaking strength of 40 lbs./inch of width, and an elongation at break of 100%.