This company planned to exhibit several new and/or expanded polymer solutions at The International Plastics Exposition, which took place March 23-27 in in Orlando, Fla. BounCell-X™ Microcellular thermoplastic polyurethane (TPU) foam contains highly elastic microcellular parts that can excel in energy absorption and cushioning applications. In addition to lightweight, superior long-term compression properties and a fast molding cycle, the material can reportedly provide a high-quality, thin skin layer that adds aesthetic values, as well as the typical advantages of TPU (e.g., outstanding abrasion and cut resistance).
Bio TPU™ is a new line of bio-based TPU made with renewable-sourced material. Bio TPU can reportedly provide the same performance and benefits as traditional petroleum-based TPU and can range in hardness from 82 Shore A to 55 Shore D.