Worthen Industries Facility Receives bluesign® System Partner Status
Worthen Industries Inc. recently announced that its Cellu Drive manufacturing facility in Nashua, N.H. has achieved bluesign® System Partner status. Worthen reportedly is one of the few U.S. facilities to achieve this status.
bluesign is a comprehensive European-based product stewardship and environmental sustainability certification for textile and allied industries. Its goal is to link chemicals suppliers, textile manufacturers, and brands together to foster a healthy, responsible, and profitable textile industry.