The HMX hot melt jet is designed for high-temperature operation. Dual independent temperature controllers for the jet and the melter allow the nozzle to be heated to specific jetting temperatures. The nozzle and syringe heaters can provide jetting temperatures up to 150°C. The HMX reportedly can reach speeds up to 200 Hz continuously, and has successfully jetted lines <0.5mm (0.019”) wide.
“The HMX has enabled PVA to develop hot melt applications used in medical, automotive and mobile electronics that would not be possible using simple needle dispensing applicators,” said Jon Urquhart, director of applications engineering.