Infrared emitters and UV lamps speed up production and improve quality for a UK-based label manufacturer.
The coating of foils, the printing of labels, or the gluing of electronic components are very different and demanding applications. However, they all require innovative production processes to maintain their appeal, durability and scratch resistance.
Great Britain-based Smith & McLaurin, a leading manufacturer and global supplier of self-adhesive labels, tags and tickets, was able to speed up and improve its production of labels by retrofitting a Heraeus Noblelight infrared system. Based in Johnstone, Renfrewshire, Smith & McLaurin sells reels of materials to printing houses and processors that manufacture finished labels and tags for a range of end users, such as supermarkets, pharmacies, logistics companies, and food-processing companies.