This company has added a new grade to its line of Vibra-Stop® non-anaerobic threadlocking/sealing products.The materials can reportedly be pre-applied to parts prior to assembly or by the user at the point of need. The new addition, Grade 19, reportedly adds the benefit of installation lubricity.