This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
Adhesives Mag logo
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Events Calendar
    • Market Trends
    • Price Adjustments
  • PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • Ask Dr. Dave
    • Strategic Solutions
    • IP in Depth
    • Tape Talk
  • TOP 20
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Photo Galleries
    • Webinars
    • Mobile App
  • EXPLORE
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
    • Take A Tour
  • MAGAZINE
    • Current Issue
    • Digital Edition
    • Advertiser Index
    • Classifieds & Services Marketplace
  • ADVERTISE
    • Contact
    • Custom Content & Marketing Services
  • SUBSCRIBE
    • eNewsletter
    • Online Registration
    • Customer Service
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Home » SONGWON: Flame-Retardant Dispersion

You have 0 Articles Left This Month. Register Today for Unlimited Access.

Adhesives and Sealants TopicsNew ProductsSustainabilityRaw Materials and Chemicals

SONGWON: Flame-Retardant Dispersion

SONGFLAME WB 201 solvent-free, aqueous, flame-retardant dispersion is designed especially for the coatings, adhesives, sealants, and elastomers (CASE) market.

January 7, 2021
KEYWORDS additives
Order Reprints
No Comments

SONGWON recently announced that it has further developed its proprietary halogen-free technology and has added a new product to its portfolio of flame-retardant synergists. SONGFLAME® WB 201 solvent-free, aqueous, flame-retardant dispersion is designed especially for the coatings, adhesives, sealants, and elastomers (CASE) market and is also suitable for textile applications requiring flame-retardant properties. The benefits of the new product reportedly include easy handling for customers working with waterborne systems, as well as low viscosity and a high active content.

“SONGFLAME® products provide a powerful building block for formulators of halogen-free materials,” said André Le Gal, leader Market Center Flame Retardants at SONGWON. “They allow our customers to achieve an ideal balance between increasingly stringent market requirements and overall cost efficiency. There has been significant progress since the launch of the SONGFLAME® range in terms of project momentum and technical approvals despite the challenging market conditions for our customers resulting from the impact of COVID-19.”

You have 0 complimentary articles left.

Register for free today to continue reading!

Already have an account? Sign in here.

Privacy Policy

Related Articles

FLEXCON: Flame-Retardant Adhesive

Clariant Flame Retardant Honored by EPA (6/16/09)

Flame Retardant by Huber Engineered Materials

Insulcast: Flame-Retardant Adhesive

Related Products

Progress in Adhesion and Adhesives, Volume 2

Progress in Adhesion and Adhesives, Volume 1

Related Directories

Huber Engineered Materials

Spartan Products Inc.

Subscribe For Free!
  • Digital Edition Subscription
  • eNewsletter
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Henkel Nicolas Krauss

Henkel Personnel Announcement Draws Massive Reader Interest

Headlines.jpg

DuPont Board Approves Separation of Nutrition & Biosciences Business through Exchange Offer

COVID-19

Are Antimicrobial Coatings Effective in the Fight Against COVID-19?

iStock-1241719830

Bonding Natural Baby Product Materials with Hot-Melt Adhesives

ASI Top 20 website

Events

February 8, 2021

Kitchen & Bath Industry Show

Virtual in 2021, the Kitchen & Bath Industry Show (KBIS) is North America’s largest trade show dedicated to all aspects of kitchen and bath design.
February 8, 2021

International Builders’ Show

Virtual in 2021 and marking its 77th year, the National Association of Home Builders (NAHB) International Builders’ Show® connects, educates, and improves the residential construction industry.

View All Submit An Event

Products

Handbook of Sealant Technology

Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

See More Products

COVER-144px

2019 Buyers' Guide

Your comprehensive buyers’ guide for raw materials, distributors, equipment, services, and finished adhesives and sealants.

The latest news and information

Content focused on adhesive & sealant manufacturing, formulations and finished products

SUBSCRIBE TODAY
  • Resources
    • List Rental
    • Ad Index
    • Classifieds & Services Marketplace
    • Want More?
    • Connect
    • Online Extras
    • Manufacturing Group
    • Privacy Policy
    • Survey And Sample
  • Subscribe
    • Digital Subscription
    • eNewsletters
    • Customer Service
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2021. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing