Palmer Holland, a North American specialty chemical and fine ingredient distributor, has announced its new distribution agreement with Zeochem. Palmer Holland will be a channel partner in the United States and Canada for Zeochem’s Purmol line of molecular sieves. Purmol powders are moisture scavengers for polyurethane coatings, adhesives, sealants, and elastomers.
Purmol adsorbents are synthetic zeolites in powder form with a complex alkali aluminosilicate structure. This structure is very open and contains pores of a regular and precisely defined size, which allows the Purmol powders to adsorb molecules selectively based on molecular size and polarity. In practice, Purmol powder absorbs water but not solvents, resins, or pigments. Its powder form allows for easy incorporation into formulations.