A team of researchers has analyzed the potential of using methyl methacrylate to bond together the structural elements of a boat.
Credit for top image: Image courtesy of Ultima_Gaina via www.gettyimages.com.
A team of researchers has analyzed the potential of using methyl methacrylate (MMA) to bond together the structural elements of a boat. The research is part of the INTERREG 2Seas Mers Zeeën research program, a European Territorial Cooperation program that covers England, France, the Netherlands, and Belgium (Flanders) with the goal of developing a 2 Seas area that protects natural resources and promotes the green economy.