Akasil® ADP 300 from BRB International is a low-viscosity silicone anti-foam compound with an active content of 100%. It has been developed specifically for non-aqueous systems.
Akasil ADP 300 has an effective foam control record at low-concentration in the following applications: electrical/electronic coating, chemical industries (adhesives, resin polymerization, etc), petroleum processing (gas scrubbing, glycol unit, etc), and formulating anti-foam emulsions.