Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEW PRODUCTS
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • EVENTS
    • ASI Academy
    • Events Calendar
  • COLUMNS
    • European Perspectives
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Classifieds
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
      • Custom Content & Marketing Services
    • CONTACT
  • SIGN UP!
Finished Adhesives and SealantsManufacturersEnd User FeaturesInfo for Electronics

Industrial Displays and Touch Panels

By Daniel Lenssen Ph.D.
October 1, 2012

Displays are omnipresent nowadays. Not only are they found in portable devices such as mobile phones and tablet PCs, but they are also used in parking ticket terminals, ticket machines, and ATMs. Display requirements have escalated as continuously as the variety of applications; users now expect complete transparency and the utmost quality.

However, liquid crystal displays (LCDs) are difficult to read in bright surroundings (e.g., in direct sunlight). The reason for this is that the displays are often covered by a glass plate to protect them against vandalism. The sunlight is partly reflected at the interfaces, and these reflections superpose the generated image. This effect can be reduced by bonding the glass cover directly to the LCD using an index-matched adhesive. For this purpose, innovative adhesives have been developed that cure by a combination of light and humidity.* Reliable curing of adhesive in shadowed areas is possible.

Bonding provides additional benefits beyond improved readability. Contamination caused by dust between the glass plates is prevented. In addition, the glass plate will not fog up in humid surroundings. The ruggedness and resistance to vibrations and shock is also increased. Typical application areas include large-area displays in the automotive, aircraft and military industries.

*Developed by DELO Industrial Adhesives.

INDEX-MATCHED LCD ADHESIVES
The refractive index of these newly developed adhesives is matched to glass, which improves the readability of the display. This circumstance is confirmed by the following calculation based on the Fresnel formulas. If a light beam vertically hits a glass surface, the formula for the reflection coefficient R is applied:

R = (nglass-nair)2 / (nglass+nair)2
Assuming reflective indices of nglass ± 1.5 and nair=1 results in a reflection of 4%, which can also be achieved if the two indices are exchanged in the formula. The result is that another 4% of light is reflected by the interface between glass and air when exiting. As shown in Figure 1, a total of three interfaces can be found at an LCD behind a protective glass plate. They reflect 4% each, totaling 12% of the surrounding light. Two of the three reflections can largely be prevented by filling the interface between the glass cover and the LCD with an index-matched adhesive. Reflections of the surface of the glass cover can further be reduced by using anti-reflective layers.

CHALLENGING REQUIREMENTS
Industrial displays are often operated by a touch panel, which means that a second bonding task must be solved. For direct LCD bonding, the adhesive used must be extremely soft. Otherwise, disturbing image effects can occur—similar to the ring patterns caused when pressing a finger onto an LCD screen. Discolorations and shadows in the corners and alongside the edges, which are called mura effects, occur if a too-hard adhesive is used. The adhesive must have a Young’s modulus far below 1 MPa to prevent these disturbing effects. The combination of extreme softness and very high transparence, yellowing stability and good adhesion even after temperature and humidity storage was a special challenge in the development of a suitable adhesive.

In addition, the glass cover is often not entirely transparent; it includes printed structures that shadow off the bonding areas and limit the use of purely UV- or light-curing adhesives. Even if the adhesive is irradiated from the side, it will not fully cure in these shadowed areas due to the restricted light penetration depth. Consequently, the adhesive remains liquid and could leak later on.

A new patent-pending solution has been developed for this bonding task.** The new chemistry combines the required adhesive properties, including softness, high optical transparence, good adhesion and yellowing stability, with the availability of a second curing mechanism. Adhesive in shadowed areas reliably cures by reacting with the air humidity.

This process is slower than fast light curing, which lasts only seconds. Curing proceeds at a speed of about 2 mm per day, which is similar to conventional silicones. However, the crucial point is that fast processing is possible due to light curing with short cycle times, and shadowed areas reliably postcure afterwards. This mechanism works even if the air humidity is as low as 20%, which means that the components can postcure at room temperature and no further curing step is necessary.

**Developed by DELO Industrial Adhesives.

BONDING PROCESSES
Two methods can be used in the bonding of industrial LCDs. The metal bezel around the display can be removed, and the glass cover can be bonded to the frameless LCD afterwards. If removal is not possible or intended, the gap between the display surface and metal bezel must be sealed with a special material before the low-viscous optically clear adhesive can be dispensed. Adhesive cannot flow into the display and damage the backlight. A bead of the high-viscous sealant is dispensed along the bezel and cured by light at the accessible areas (see Figure 2). The second curing mechanism ensures that adhesive flown into the gap is reliably humidity-cured.

The adhesive is also suitable for another process. A “dam” is dispensed onto the bezel and cured before dispensing the optically transparent adhesive (see Figure 3). The dam defines the layer thickness while tack prevents shifting of the glass cover that is laid on at the end of the process.

The optically transparent adhesive, called fill, is dispensed onto the display in a defined pattern that must be adapted to the display size and bezel height. Optimized dispensing parameters allow reproducible and bubble-free joining. Finally, the glass cover is attached either parallel to the LCD, or it is put down on one edge and then tilted down. As soon as the adhesive has spread, it can be cured. Adhesive in shadowed areas cures outside the production line by means of the second humidity curing mechanism.

YELLOWING RESISTANCE AND OPTICAL TRANSPARENCY
The key requirement of the adhesive is high transparency. The transmission of a 0.5 mm layer is more than 98% in the entire visible spectrum (see Figure 4). The yellowing stability was verified in accelerated sunlight tests.

As the adhesive must be extremely soft, the adhesion values are rather low. Figure 5 shows typical adhesion values in the stud pull test. For this test, two elongated glass plates are bonded to form a cross of an area of 25 x 25 mm2. The plates are then pulled apart vertically to the bonding area. The resulting forces remain constant even after humidity storage and are sufficient for large-area bondings. For a 10.4 in. display, a stud pull force of 0.5 MPa results in a release force of more than 1,600 kg.

Typical refractive indices are around 1.47. This is very close to the values of glass (e.g., quartz glass with 1.46), and typical values of cellulose acetate (triacetate or TAC film) with 1.48. This is the material used as polarization film of the LCD, which is the actual surface to be bonded.

Table 1 shows typical parameters. The first adhesive is a high-viscous material to be used as sealing or dam. Three soft, optically clear adhesives for direct LCD bonding are also listed. The first one is purely light-curing, the second one is dual-curing, and the third one is a dual-curing product with further optimized yellowing resistance. The last adhesive on the right is somewhat harder. It gives improved adhesion to plastic and is suitable for bonding PMMA covers.

A BETTER DISPLAY
A completely new chemistry has been developed with the new adhesives: dual curing by light and humidity. Used in industrial displays and touch panels, the optically transparent, yellowing-resistant and soft materials are ideal for large-area display bonding.


 For more information, contact DELO Industrial Adhesives at (978) 254-5275, info@delo.us or www.delo.us. 

KEYWORDS: adhesives in electrical/electronic

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Daniel Lenssen, Ph.D., serves as Product Manager for DELO Industrial Adhesives.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • linked network nodes

    Using the Power of AI for Adhesive and Sealant Formulation

    With the help of software solutions, adhesive formulators...
    Finished Adhesives and Sealants
    By: Karen Parker
  • ASI top 20 global manufacturers

    2025 ASI Top 20: Leading Global Adhesives and Sealants Manufacturers

    ASI's annual ranking of the top 20 global adhesive and...
    Adhesives and Sealants Topics
    By: Karen Parker
  • science test tubes

    2026 Adhesives and Sealants Raw Materials Roundup

    After more than two years of contraction, the...
    Raw Materials and Chemicals
    By: Karen Parker
Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

Image of a blue bar chart with arrow pointing up

Iran War and Logistics Challenges Impact Adhesives and Sealants Pricing

news on internet screen

H.B. Fuller and Ancora Holdings Clash Over Proposed Medical Adhesives Acquisition

Aerial picture of a chemical facility

DELO Reports Record Revenue for Fiscal Year

ASI Top 20 website

Events

June 15, 2026

Adhesive and Sealant Council Executive Leadership Conference

This annual event provides current and future leaders in the adhesives and sealants industry with the opportunity to expand their knowledge and network with peers.

September 14, 2026

Women in Chemicals Conference

Organized by Women in Chemicals, this landmark conference will offer opportunities for networking, learning, and professional development. With a diverse array of sessions, workshops, and social events, participants can expect a dynamic program designed to empower and inspire.

View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

ASI CASE EBOOK

ASI raw materials roundup

Related Articles

  • Industrial Displays and Touch Panels

    See More
  • Case Study: Adhesive Promotes Unbreakable Displays in Automotive Applications

    See More
  • 3M TOUCH SYSTEMS INC.: Large-Format Touch Screens

    See More

Related Products

See More Products
  • 4.png

    Progress in Adhesion and Adhesives, Volume 7

  • wood adhesives.jpg

    Wood Adhesives

  • thirdedition.jpg

    Handbook of Adhesive Technology, Third Edition

See More Products

Related Directories

  • Composite Panel Association

×

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing