ITW TACC: Subfloor Adhesive
LUMBER LOCK G Subfloor and Construction Adhesive provides durable, weatherproof bonds, adhering to wet and frozen lumber while helping keep job sites clean with low-splattering performance. This product also meets SCAQMD Rule 1168 air quality requirements and contributes to several credits for many green building rating systems, including LEED®.
Like its established solvent-based counterpart LUMBER LOCK, LUMBER LOCK G is third-party tested to meet ASTM D3498 Field-Gluing Plywood to Lumber Framing for Floor Systems. LUMBER LOCK G comes in 28 oz cartridges and 55-gallon drums. Green building and product data can be found online in ITW TACC’s Document Library.
For more information, visit www.itwtacc.com.
Like its established solvent-based counterpart LUMBER LOCK, LUMBER LOCK G is third-party tested to meet ASTM D3498 Field-Gluing Plywood to Lumber Framing for Floor Systems. LUMBER LOCK G comes in 28 oz cartridges and 55-gallon drums. Green building and product data can be found online in ITW TACC’s Document Library.
For more information, visit www.itwtacc.com.
Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!