Clariant and Omya Develop Label-Free Innovation for SMP Sealants
Clariant and Omya joined forces on a new project to tackle concerns surrounding the yellowing of the increasingly popular silane modified polymers (SMP) sealants. The results of their collaboration addressed the yellowing issue while delivering a label-free solution with higher light and heat performance versus standard solutions in the market. The partners introduced AddWorks IBC 760 to visitors at the European Coatings Show 2023.
SMP is one of the industry’s fastest-growing sealant technologies for diverse construction, automotive, and component applications. Delivering high-performance elastic bonding on multiple substrates, these reactive sealants can be painted unlike other technologies, and they are free of solvents and isocyanates. However, using heat and light stabilizers for weathering performance has traditionally caused unsightly yellowing both in-cartridge and temporarily on extrusion, many are based on hazard-labeled materials, and service life for SMP sealants is still limited.