An innovative, ecofriendly glue designed by a Cal Poly chemistry research team in collaboration with an East Coast company has been approved for a United States government patent. The patent creates a pathway for proprietary commercial production of the glue innovation under the direction of the Massachusetts-based company Geisys Ventures.
The new adhesive, which will be formally known as D-Glue, for "debondable glue,” was created by Cal Poly chemistry professor Phil Costanzo and Geisys Ventures CEO, Kris Stokes.