Scott Bader ATC Begins Structural Adhesive Production in North America
Scott Bader ATC, based in Drummondville, Canada, has begun manufacturing and supplying Crestabond structural adhesives in North American. After months of installation and testing, the first batch of Crestabond M1 structural adhesive has been successfully produced and delivered to customers.
The expansion of Crestabond production to Scott Bader ATC, a €2.2 million investment, will reportedly allow Scott Bader to meet the growing demand for its MMA primerless structural adhesives within the North American market. It will also significantly reduce transport emissions and delivery times, helping Scott Bader to deliver a faster, more efficient service for its customers with less environmental impact.