Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEW PRODUCTS
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • EVENTS
    • ASI Academy
    • Events Calendar
  • COLUMNS
    • European Perspectives
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Classifieds
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
      • Custom Content & Marketing Services
    • CONTACT
  • SIGN UP!
Converting/PackagingSustainabilityRaw Materials and Chemicals

Is it Time to Decouple from Petroleum?

Bio-polymers have entered the market, and demand is expected to grow rapidly over the next decade.

By Steven Gailbreath, Marc Jackson
bio-based raw materials for adhesives
What is the reason for continued interest in bio-based materials?
fully recyclable Coca-Cola bottle
Coca-Cola has introduced a fully recyclable alternative to the traditional PET plastic bottle shown here. (Photo courtesy of The Coca-Cola Co.)
table 1 general formulation
Table 1. General Formulation
bio-based raw materials for adhesives
fully recyclable Coca-Cola bottle
table 1 general formulation
August 1, 2010
In May 2009, The Coca-Cola Co. unveiled its new package. According to the press release, the PlantBottle™ is fully recyclable, has a lower reliance on non-renewable resources, and reduces carbon emissions compared with polyethylene terephthalate (PET) plastic bottles. The rest of the press release discusses the environmental virtues of the new package, but dialogue with Coke employees revealed a different (though equally important) driver: “We have been in business for over 100 years and we plan to be in business for over 100 more years. We are taking steps now to reduce our dependence on petroleum-based raw materials.”

Bio-polymers have entered the market, and demand is expected to grow rapidly over the next decade. According to the European Polysaccharide Network, capacity for bio-based plastic will increase from 0.36 million tons in 2007 to 2.33 million tons in 2020, and some companies are taking this opportunity to introduce new products. For example, Innovia has reinvented cellulosic film with its Natureflex™ line. Coatings and engineering improvements, coupled with a recently capitalized production line, have put this mature product back on a growth track. Corn-derived polylactic acid (PLA) from NatureWorks LLC, a Cargill company, (and others) and Novamont’s Mater-Bi™ are used for films, molded parts, and a variety of other applications.

These are only a few examples of the widespread advent of bio-based industrial raw materials and finished products. We have all heard the adage, “Sure, I want to be environmentally responsible, but not if it costs more money.” Despite this sentiment, the unit costs of the products listed in the preceding examples range from two to five times more than their petrochemical predecessors. So what is the reason for the continued interest in bio-based materials?
 

It's Environmental Altruism, Right?

According to many, new carbon is better for the environment than old carbon. Vinçotte, developers of the OK Biobased certification labeling system, explains the significance of bio-based material in the documentation on its website. In summary, the consumption and release of new carbon does not lead to an increase in the average amount of CO2 present in the atmosphere. This, the theory goes, helps to reduce the warming effect caused by greenhouse gas emissions.

Despite the atmospheric advantages of renewable materials, not everyone is ready to commit to changing. For example, renewability is not yet part of the Wal-Mart packaging scorecard. GreenerPackage.com, Wal-Mart’s packaging data partner, says it is waiting until the Federal Trade Commission provides guidance on what constitutes a renewable resource in the next version of the Environmental Marketing Claims guideline, which is projected to be available sometime in 2010.

Still, the interest in bio-based raw materials persists and has begun to translate into real demand. Frito-Lay and International Paper are two global corporations that recently added bio-based offerings to their traditional product lines (in the form of compostable snack food bags and PLA-coated hot beverage cups, respectively). The desire to improve the reliability and availability of raw materials is driving the move to bio-based raw materials as much-or more-than environmental considerations.

The reliability of petroleum-based adhesive resins has been impacted by fundamental shifts in the global chemical supply infrastructure. New and efficient ethylene production has been installed in the Middle East. As these plants come on-stream, older and smaller facilities in the U.S. and Western Europe are shutting down. Most of the new plants are designed to crack natural gas instead of naphtha and thus will not generate the pyrolysis gasoline byproduct needed as the feedstock for many hydrocarbon products like isoprene and tackifying resins.
 

Can the Adhesive Supply Chain Decouple?

Fortunately, adhesive producers and suppliers are taking steps to offer alternatives to help improve supply-chain diversification. Choices are available for companies that range in size and scope from global adhesives producers that are interested in large volume and consistent quality for multiple production locations, to specialty adhesive manufacturers that are locked into long-term formulations, to all of those in between.

The list of products based on sustainable materials is growing, and chemistries are available that use raw materials that are renewable within our lifetimes. The adhesive formulators’ expertise allows them to develop products that achieve the required performance while meeting the demands of their and their customers’ supply chain professionals.

Polymers
Polymers give adhesives structure, and the choice of polymers depends on the final end-use application. One particular polymer building block that has experienced supply challenges over the past several years has been isoprene. Isoprene is used to produce polymers for a variety of applications ranging from toothbrush handles to high-performance, engineered pressure-sensitive adhesives. Suppliers of isoprene-based polymers recognize their customers’ sensitivity to the supply volatility, and they are taking steps to develop alternatives.

In addition, many of these same companies are developing polymers based on bio-isoprene, a polymer building block that is manufactured from oilseed waste. In December 2009, Goodyear, in partnership with Genencor, announced the introduction of the world’s first concept demonstration tire based on bio-isoprene technology. Although this technology is still several years from commercial production, Goodyear’s Jesse Roeck summarized the potential of the technology, saying “The development of BioIsoprene™ could make Goodyear less dependent on oil-derived products. We share Genencor’s vision of lessening industry impact on the environment by applying renewable raw materials in the supply chain.”

Polymers in commercial quantities are available for packaging adhesive producers today. For example, NatureWorks produces biopolymers derived from renewable resources. DaniMer Scientific, LLC has taken these polymers one step further; its adhesive developed for packaging applications contains over 99% renewable content.

Oils and Waxes
Oils and waxes are used in adhesives as performance modifiers and processing aids. Many of the products traditionally used in adhesives are subject to disruptions due to petroleum dynamics. Produced as a bottom-stream in the fractional distillation of petroleum, paraffin wax can be captured and further processed to be used in the gasoline pool. As gas prices rise, paraffin waxes become less available. Vegetable oil companies, such as Cargill, are also working on corn- or soy-based oil and wax replacements as alternatives.

Resins
Tackifying resins improve specific adhesion to a variety of substrates. Hydrocarbon tackifiers are manufactured from the byproducts of ethylene and propylene production. When they were originally introduced, hydrocarbon resins were offered as synthetic alternatives to naturally derived resins. At the time, it made sense because they were cheaper and readily available. With more companies focusing on long-term supply sustainability, bio-based resins are now back in vogue as natural alternatives to synthetic resins.

Today, rosin offers a raw materials source that is commercially available in the scale needed and has a positive long-term supply outlook. Rosin’s ester derivatives, rosin esters, are of particular importance in adhesive applications.
 

Multiple Options

Of course, decoupling is not an all-or-nothing proposition. Replacing just a portion of your adhesive with a supply sustainable alternative helps to reduce your risk. The example formulation shown in Table 1 illustrates how a hot-melt pressure-sensitive adhesive can be economically diversified from what has typically been 0% bio-renewable content (BRC) to nearly 50% BRC. By incorporating a bio-isoprene polymer or a naphthenic oil alternative, the BRC can be pushed even higher.

Industrial companies are planning for a post-petroleum economy. Bio-based raw materials are available for adhesive companies today, and it is likely that the quality, range, and availability of these products will continue to increase.
 



Editor’s note: PlantBottle™ is a trademark of Coca-Cola; Natureflex™ is a trademark of Innovia; Mater-Bi™ is a trademark of Novamont; BioIsoprene™ is a trademark of Genencor; Kraton™ is a trademark of Kraton Performance Polymers; Nyflex™ is a trademark of Nynas; Sylvalite® and Sylvares® are registered trademarks of Arizona Chemical.
 



For more information, contact Arizona Chemical Co. at 4600 Touchton Road E., Suite 1500, Jacksonville, FL 32246; call (800) 526-5294; e-mail info@azchem.com; or visit www.arizonachemical.com.

KEYWORDS: bio-based materials flexible packaging food/beverage rigid packaging

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Steven Gailbreath is upgrade market manager, Americas, for Arizona Chemical Co.
Marc Jackson is president of Teckrez. He previously held positions with Melrob Ltd. and Arizona Chemical Co.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • linked network nodes

    Using the Power of AI for Adhesive and Sealant Formulation

    With the help of software solutions, adhesive formulators...
    Raw Materials and Chemicals
    By: Karen Parker
  • ASI top 20 global manufacturers

    2025 ASI Top 20: Leading Global Adhesives and Sealants Manufacturers

    ASI's annual ranking of the top 20 global adhesive and...
    Finished Adhesives and Sealants
    By: Karen Parker
  • science test tubes

    2026 Adhesives and Sealants Raw Materials Roundup

    After more than two years of contraction, the...
    Sustainability
    By: Karen Parker
Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

Image of a blue bar chart with arrow pointing up

Iran War and Logistics Challenges Impact Adhesives and Sealants Pricing

news on internet screen

H.B. Fuller and Ancora Holdings Clash Over Proposed Medical Adhesives Acquisition

Aerial picture of a chemical facility

DELO Reports Record Revenue for Fiscal Year

ASI Top 20 website

Events

June 15, 2026

Adhesive and Sealant Council Executive Leadership Conference

This annual event provides current and future leaders in the adhesives and sealants industry with the opportunity to expand their knowledge and network with peers.

September 14, 2026

Women in Chemicals Conference

Organized by Women in Chemicals, this landmark conference will offer opportunities for networking, learning, and professional development. With a diverse array of sessions, workshops, and social events, participants can expect a dynamic program designed to empower and inspire.

View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

ASI CASE EBOOK

ASI raw materials roundup

Related Articles

  • GettyImages-175259975.jpg

    Is It Time to Diversify Your Product Line?

    See More
  • Alternative mixing strategies

    Is it Time to Upgrade Your Mixer?

    See More
  • Toll Processing: Is It Right for You?

    See More

Related Products

See More Products
  • Optimizing Social Media from a B2B Perspective

  • How to Formulate & Test Sealants (Virtual Course 9/23/26)

  • How to Formulate & Test PSAs (Virtual Course 6/17/26)

See More Products

Related Directories

  • Ingredients + Specialties from Univar Solutions

    Ingredients + Specialties from Univar Solutions, a global provider of specialty ingredients and chemicals, serves the coatings, adhesives, sealants, and elastomers markets, including solutions for other performance materials. We empower our customers and suppliers with specialty ingredients, solutions, and technical expertise through our global Solution Centers, focusing on CASE industry innovations.
  • R.E. Carroll Inc.

    Specialty chemical and petroleum products distributor specializing in LTL raw materials and packaged petroleum products from six strategically located warehouses in California, Georgia, Illinois, Pennsylvania, Ohio, and Texas.
×

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing