BOSTIK AND POLYTEC PT: Thermal Conductive Adhesives
Bostik and Polytec PT are launching a new range of thermal conductive adhesives (TCA) to address the challenge of thermal management in the latest cell-to-pack (CTP) battery design for e-mobility solutions.
Thermal management is vital to ensure the operating temperature of EV-battery systems remains between 20 °C and 40 °C for optimum battery life and performance. Thermal interface materials (TIM) such as TCAs are essential to battery design to ensure a robust thermal connection between the battery/cell environment and the cooling elements. With the trend towards fast charging for e-mobility, the importance of thermal management and TIMs is increasing significantly.