Arkema Lowers the Carbon Footprint of Its Bio-Based Polyamide 11 Chain

Arkema's Rilsan polyamide is derived from renewable castor seeds. Photo courtesy of Arkema.
Arkema further decreased the carbon footprint of its bio-based Rilsan® polyamide 11 by 46% reaching less than 2 kg CO2e/kg, by using renewable or low carbon energy sources and by making energy efficiency improvements in its production sites. It represents an improvement of around 70% relative to traditional polyamide resins using fossil-based raw materials.
Derived from renewable castor seeds, Rilsan polyamide 11 is 100% segregated bio-based. The amino 11 monomer and the downstream polymers are produced using low carbon and renewable energy – both in terms of electricity and combustible fuels. Arkema recently announced a biomethane supply agreement with ENGIE in France and carried out several energy efficiency improvements in its polyamide 11 chain production sites over the last year.
“This is an important step for our customers and the markets we serve,” said Erwoan Pezron, senior vice president, Arkema’s High Performance Polymers. “The lower carbon footprint we announce today applies to our entire global production, not just a particular set of grades or a certain location. This allows our customers to deliver on their commitment to decarbonize and to develop more sustainable products at scale. Furthermore, we have a strong action plan in place to further decarbonize this range, with a 2030 target to reduce the carbon footprint by a further 50%. Our objective is to continue to offer our customers high- performance materials with one of the lowest carbon footprints in the market.”
To learn more, visit www.arkema.com.