HENKEL: Cold Rebuilding Epoxy Material for Automotive Body Repair
Henkel reports that Teroson EP 5020 TR can be applied at room temperature in a smooth, flameless, and solder-free process.
Henkel recently introduced Teroson EP 5020 TR, a two-component epoxy-based cold rebuilding material designed to replace conventional tin solder in aftermarket repairs of automotive body damages. Fast curing, easier to sand, and smoother to apply than previous solutions, the material also reportedly eliminates the heat and open flame process required for tin-soldered repairs.
As the automotive industry continues to develop new body materials, there is a need for compatible aftermarket repair technology that has no impact on adjacent plastic components, paint, or backside corrosion protection. Henkel reports that Teroson EP 5020 TR can be applied at room temperature in a smooth, flameless, and solder-free process.