Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEWS
    • Latest Headlines
    • ASI News Now
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • NEW PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • From the Editor
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • EVENTS
    • ASI Academy
    • Events Calendar
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • DIRECTORIES
    • Buyers' Guide
    • Equipment Handbook
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Sponsor Insights
    • Classifieds
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
    • CONTACT
  • JOIN!
Home » Topics » Columns » Q&A About Polyurethanes

Q&A About Polyurethanes
Q&A About Polyurethanes RSS Feed RSS

Q&A About Polyurethanes

Consistent Performance in a Waterborne Polyurethane Adhesive

What should we do about inconsistent performance in a waterborne polyurethane adhesive?
Dr. Jeffrey F. Dormish
May 1, 2017
Scaling up products from the laboratory to field trials to full production can often be problematic, whether a new polymer is being developed or a formulated finished adhesive is manufactured. If bond failures are occurring during production, the plant may go back to the adhesive supplier and claim the adhesive is at fault.
Read More
Q&A About Polyurethanes

What type of raw materials should be considered in formulating products with a bio-based focus?

A definition of “bio-based” is a good starting point for this discussion.
Dr. Jeffrey F. Dormish
March 1, 2017
A definition of “bio-based” is a good starting point for this discussion. The U.S. Department of Agriculture (USDA) defines bio-based products as those derived from plants and other renewable agricultural, marine, and forestry materials. Standardized tests have been developed (ASTM D 6866) to quantify the bio-based content of a product or a raw material.
Read More
Q&A About Polyurethanes

What types of surface preparation are necessary to obtain strong and durable bonds?

Having a clean surface is a key requirement to obtain a strong and reliable bond.
Dr. Jeffrey F. Dormish
September 1, 2016
Companies using adhesives are expected to be able to consistently produce an assembly―whether in the flexible packaging, furniture, automotive or construction industry―without differences in the quality of the product manufactured. This is the case for both high-performance structural bonds and applications with lower performance requirements.
Read More
Q&A About Polyurethanes: What types of chemical structures could be built into a polyurethane adhesive to optimize heat resistance?
Q&A About Polyurethanes

What types of chemical structures could be built into a polyurethane adhesive to optimize heat resistance?

Formulation recommendations can be made to address each aspect of thermal stability.
Dr. Jeffrey F. Dormish
May 2, 2016
What types of chemical structures could be built into a polyurethane adhesive to optimize heat resistance? Can you make any formulation recommendations?
Read More
Polyaspartic Coatings
Q&A About Polyurethanes

Polyaspartic Coatings

The polyaspartic coatings technology has been available since the 1990s and is an extension of polyurethane chemistry.
Dr. Jeffrey F. Dormish
March 1, 2016

I work in the technical department developing coatings based on various polymer backbones. I am familiar with typical polyurethane raw materials, but have recently become aware of polyaspartic coatings. Could you provide an overview of this technology?


Read More

Q&A About Polyurethanes

What are the advantages of using polyurethane technology for hot-melt applications?
Dr. Jeffrey F. Dormish
September 1, 2015

I am familiar with traditional ethylene vinyl acetate (EVA), polyester and polyamide (PA)-based hot-melt adhesives. What are the advantages of using polyurethane technology for hot-melt applications?


Read More

Q&A About Polyurethanes: Formulating Basics for Coatings

What are some fundamental issues that I should know regarding the basics of formulating coatings?
May 1, 2015

An important concept to learn is critical pigment volume concentration (CPVC). Understanding this concept is essential for formulating high-performance coatings. In fact, it’s an “elephant in the room” for many formulators—ignored at our peril.


Read More

Q&A About Polyurethanes: Raw Materials Storage Issues

How should polyurethane and polychloroprene raw materials be stored to optimize their shelf life?
Dr. Jeffrey F. Dormish
March 2, 2015

I am an adhesives manufacturer and, as business is increasing, I have a need for a larger warehouse for the polyurethane and polychloroprene raw materials used. How should these raw materials be stored to optimize their shelf life?


Read More

Q&A About Polyurethanes: Coatings Raw Materials

Can you provide some general information regarding coatings raw materials?
Dr. Jeffrey F. Dormish
September 2, 2014

I am familiar with formulating polyurethanes for adhesive applications, but would like to learn more about coatings raw materials in order to provide a broader product profile to my customers. Can you provide some general information?


Read More

Q&A About Polyurethanes: Increasing Market Requests for Sustainable Adhesives

How is the adhesive industry addressing market requests for increased sustainability?
Dr. Jeffrey F. Dormish Heinz-Werner Lucas
May 1, 2014

Researchers have identified a number of global trends that will have an impact on the adhesive business. One major trend is to use energy more efficiently—both to protect the environment by reducing carbon emissions and from a basic cost-of-energy standpoint.


Read More
Previous 1 2 Next
Manage My Account
  • Join Adhesives & Sealants Industry
  • Manage My Preferences
  • Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Industrial robot performing plasma surface treatment on an automotive component
    Sponsored byPlasmatreat North America

    Engineering the Molecular Interface: Atmospheric Plasma Cleaning and Activation for Reliable Bonding

  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

news on internet screen

H.B. Fuller Announces Seven Site Closures

news on internet screen

Ancora Calls for Potential Sale of H.B. Fuller

Photo of a person holding a tablet, reading a new story

H.B. Fuller Rejects Ancora’s Second Offer for Building Adhesive Solutions Business

ASI 2026 Top 20 Adhesives & Sealants List

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Adhesives Technology Handbook   3rd Edition

Adhesives Technology Handbook 3rd Edition

See More Products

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing