Independent Machine Co. of Fairfield, NJ, has developed its latest system for slitting and traverse winding pressure sensitive adhesives, tapes and foam.
EFD has introduced a new type of benchtop fluid dispenser that uses positive displacement technology to apply accurate, consistent amount of 2-part epoxies and other assembly fluids that change viscosity during the dispensing process.
TRA-BOND 789-3 is a high-strength, one-component adhesive designed for applications in the microelectronics industry that require good moisture resistance, like package sealing and substrate attach.
A new Filter-Regulator-Manifold (FRM) assembly kit from Nordson Corp. contains all of the parts required to supply the correct volumes of factory air to Nordson piston pump adhesive melters and pneumatic dispensing guns
Speedline Technologies, Inc. has announced that its MPM Gel-Flex conformal board support system reduced set up time by 50 percent in customer beta testing