Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • NEW PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • From the Editor
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • EVENTS
    • ASI Academy
    • Events Calendar
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Classifieds
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
    • CONTACT
  • SIGN UP!

Plasma Treatment Boosts Adhesion

May 1, 2004
Low-pressure vacuum plasmas have typically been used to treat two- and three-dimensional plastic objects and polymer films. However, the recent introduction of high-density atmospheric plasma for film, foil, paper, foam, nonwoven and woven substrate applications has had a significant impact on the surfaces of these materials at considerably lower capitalization costs.

Close-up of a side view of plasma being discharged at the electrode of the treater.


You may already know something about the benefits of plasma treatment, such as higher treatment (dyne) levels, extended life of treatment over time, the lack of surface morphology degradation, and the elimination of pinholing and backside treatment.

Until recently, low-pressure vacuum plasmas have been used to treat two- and three-dimensional plastic objects and polymer films. The recent introduction of high-density atmospheric plasma for film, foil, paper, foam, nonwoven and woven substrate applications has had a significant impact on the surfaces of these materials at considerably lower capitalization costs.

High-density atmospheric plasma represents a new generation of surface-treatment technology. It allows plasmas to be sustained at atmospheric pressure in a way that permits the surface treatment of polymers and other substrates. It can be configured to work with a variety of feeding systems, including continuous web.

Corona

How does Plasma Compare to Corona?

Corona treatment is an electrical process that uses ionized air to increase the surface tension of non-porous substrates. Normally, corona-treating systems operate at an electrical voltage of approximately 10 kV.

Like corona, plasma is the electrical ionization of a gas. The plasma (glow) discharge creates a smooth, undifferentiated cloud of ionized gas with no visible electrical filaments. However, unlike corona, plasma is created at much lower voltage levels and temperatures.

Plasma

Plasma Effects on Substrate Surfaces

Corona converts the substrate surface from a non-polar state to a polar state. Oxygen molecules from the corona discharge area are then free to bond to the ends of the molecules in the substrate being treated, resulting in an increase in surface tension.

The same description holds true for atmospheric plasma, with a few exceptions. The rate at which electron bombardment occurs within a high-density atmospheric plasma is up to 100 times greater. This increased electron activity forces greater ion bombardment to the substrate surface. This results in increased etching, chain scission and crosslinking on the substrate's surface, which influences stronger bonding attributes across the surface of the web. Specifically, mechanical interlocking is enhanced, bonding materials together by allowing the adhesive or sealant to take advantage of the microscopic roughness etched to the surface by atmospheric plasma, locking them together. In addition, covalent chemical bonding is promoted, using mutually reactive chemical groups newly resident at the substrate surface (delivered by atmospheric plasma treatment) and the adhesive to form the strongest, most durable bond.

Summarizing the treatment process, high-density atmospheric plasma employs chemical gases that produce controlled chemical reactions on the surface. Chemistry molecules that are introduced are propelled to the material surface. Low-molecular-weight material is cleaned from the surface and specific gas molecules covalently bond to the surface. This is how adhesion can be boosted between the adhesive and the material surface.

Atmospheric plasma technology also eliminates the possibility of backside treatment. The high-speed photos capture the optical differences between corona and atmospheric plasma treatment. The corona image shows the expected "filaments," while the plasma treatment generates a smooth treat pattern.

Plasma3 Atmospheric Plasma System.

Benefits of Atmospheric Plasma for Adhesive Adhesion

Plasma treatment offers three key benefits that adhesive manufacturers can use to their advantage.

1. Longer life treatments. Substrates that have been atmospheric plasma-treated hold their treatment levels longer than corona-treated surfaces. Longer treatment life allows product converters to take advantage of economies of scale during production, increase inventory life and provide enhanced manufacturing flexibility.

2. Higher treat levels allow for treatment of difficult-to-treat surfaces. Atmospheric plasma treatment is a viable alternative for substrates for which corona treating is ineffective. For example, difficult-to-treat fluoropolymer-based materials like Teflon® do not respond to the corona process but do respond to atmospheric plasma treatment.

3. Treatment of thicker substrates. While substrates that are thicker than 0.125" usually do not respond well to the corona process, they can be treated by atmospheric plasma. Films, metallized films, foils, foams, wovens and nonwovens are all candidates for atmospheric plasma surface treatment.

An atmospheric plasma treatment system called Plasma3™ that can operate at low temperature to provide the advantages plasma technology has over existing surface-treatment technologies has been developed by Enercon Industries. The surface energies of materials treated by this system have been shown to increase substantially, thereby significantly enhancing the wettability, printability and adhesive/ink/coating adhesion properties of these materials.

Web-Based Atmospheric Plasma Market Applications

Water- and solventborne, alcohol-based, and cold-seal adhesives are used for a variety of laminating applications. They are used by contract laminators and consumer products companies to bond multiple combinations of film, fiberglass, foam, fabric, paper, nonwovens, and rubber. The laminates are used to produce a range of products, including the following.

  • Packaging applications - sealing tapes, weather-strip, labels
  • Automotive applications - seals, gaskets, headliners, trim
  • Textile applications - protective apparel, outerwear
  • Medical applications - medical drapes and garments, bandages, electrodes, labeling, lidding, covers
  • Electronic applications
  • Bonding/assembly and thermal management tapes

The system also has the flexibility to be operated with variable chemistries and without the generation of ozone, pin-holing, and backside treatment.

For more information, contact Rory Wolf at rwolf@enerconmail.com .

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • 2026 ASI Top 20: Leading Global Adhesives and Sealants Manufacturers

    2026 ASI Top 20: Leading Global Adhesives and Sealants Manufacturers

    Every year, we study the leading worldwide manufacturers...
    Adhesives and Sealants Topics
    By: Karen Parker
  • PSA Market

    Trends and Opportunities in Pressure-Sensitive Adhesives: Sustainability, Innovation, and Market Growth

    The pressure-sensitive adhesives market is growing...
    Pressure-Sensitive Adhesives (PSAs)
    By: Chirag Tripathi and Parag Shah
  • science test tubes

    2026 Adhesives and Sealants Raw Materials Roundup

    After more than two years of contraction, the...
    Raw Materials and Chemicals
    By: Karen Parker
Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

Photo of a person holding a tablet, reading a new story

FTC Successfully Blocks Henkel’s Acquisition of Liquid Nails

Image of a computer keyboard with the letters N E W S highlighted

H.B. Fuller Receives BAS Acquisition Proposal as AMS Deal Proceeds

news on internet screen

H.B. Fuller Board Rejects Unsolicited Proposal for Building Adhesives Solutions Business

ASI 2026 Top 20 Adhesives & Sealants List

Events

September 15, 2026

Coatings Trends & Technologies Summit

This annual Midwest coatings conference combines all of the high-quality technical presentations, exhibits and networking opportunities from the Coatings Trends and Technologies and Powder Coating Summit conferences into one new event. The event caters to both liquid and powder coatings formulators and manufacturers.

September 16, 2026

World Adhesive & Sealant Conference (WAC) 2026

As the industry’s premier international event, WAC 2026 offers a unique opportunity for professionals from every continent to connect, collaborate, and shape the future of the sector.
View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

Related Articles

  • Picture of a Robafoam robot dispensing foam sealant

    Plasma Treatment Increases Adhesion Reliability of Foam Sealing

    See More
  • NORDSON MARCH: Plasma Treatment System

    See More
  • Applications For Plasma Surface Treatment In The Medical Industry

    See More

Related Products

See More Products
  • Handbook of Adhesion, 2nd Edition

  • 4.png

    Progress in Adhesion and Adhesives, Volume 7

See More Products

Related Directories

  • Enercon Industries Corp.

    Offers atmospheric plasma and flame surface treating to improve surface adhesion of plastics, composites, glass, and metals. Applications for plasma treaters include assembly, coating, potting, and bonding. Plasma & flame in-line pretreatment technologies improve adhesive bonds and quality, while eliminating the need for hazardous primers and manual surface prep methods.
×

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing