Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEWS
    • Latest Headlines
    • ASI News Now
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • NEW PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • From the Editor
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • EVENTS
    • ASI Academy
    • Events Calendar
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • DIRECTORIES
    • Buyers' Guide
    • Equipment Handbook
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Sponsor Insights
    • Classifieds
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
    • CONTACT
  • JOIN!
Home » Topics » Columns » Ask Dr. Dave

Ask Dr. Dave
Ask Dr. Dave RSS Feed RSS

Ask Dr. Dave

Do reactive acrylics and anaerobics behave like epoxies in terms of curing?

Dave Dunn's March 2017 column.
Dave Dunn, Ph.D.
Dave Dunn Ph.D.
March 1, 2017
Do reactive acrylics and anaerobics behave like epoxies in terms of curing and properties like heat resistance?
Read More
Ask Dr. Dave

What is the difference between a hardener, a primer, an accelerator, and an activator?

Dave Dunn's February 2017 column.
Dave Dunn, Ph.D.
Dave Dunn Ph.D.
February 1, 2017
What is the difference between a hardener, a primer, an accelerator, and an activator for adhesives and sealants?
Read More
Ask Dr. Dave

What has been your experience using silicone caulks, both interior and exterior?

Dave Dunn's December 2016 column.
Dave Dunn, Ph.D.
Dave Dunn Ph.D.
December 1, 2016
Longtime readers of this column may note that I have always been a fan of silicone sealants; however, I worked for a manufacturer of these materials for many years, so I hope I can be totally objective. I have no doubt that the durability and longevity of silicones cannot be exceeded in most applications. However, I can offer you several observations from my personal experience using them at home.
Read More
Ask Dr. Dave

What tips can you provide for bonding plastics and composites with adhesives?

Dave Dunn's November 2016 column.
Dave Dunn, Ph.D.
Dave Dunn Ph.D.
November 3, 2016
Adhesives are often a better way to assemble plastics than by using mechanical assembly with fasteners. For example, fiberglass composites are routinely bonded with epoxy or reactive acrylic adhesives in the automotive and marine industries because they give high strength and durable bonds.
Read More
Ask Dr. Dave

Why use pressure-sensitive tape adhesives in the assembly of electronic devices?

Dave Dunn's October 2016 column.
Dave Dunn, Ph.D.
Dave Dunn Ph.D.
October 3, 2016
What are the pros and cons of using pressure-sensitive tape adhesives in place of liquid adhesives in the assembly of electronic devices?
Read More
Ask Dr. Dave

What alternatives do I have for bonding to surfaces like polyethylene and polypropylene?

Dave Dunn's September 2016 column.
Dave Dunn, Ph.D.
Dave Dunn Ph.D.
September 1, 2016
What alternatives do I have for high-strength bonding to surfaces like polyethylene and polypropylene?
Read More
Ask Dr. Dave

How should we prepare our surfaces for adhesive bonding?

Dave Dunn's August 2016 column.
Dave Dunn, Ph.D.
Dave Dunn Ph.D.
August 1, 2016
This is a very broad topic for this column. Adhesive bonding requires several choices to be made, such as type of adhesive, additives like adhesion promoters and surface preparation.
Read More
Ask Dr. Dave

What options do we have for high-performance liquid gaskets?

The most common types of liquid gaskets are RTV silicones and anaerobics.
June 1, 2016
Question: What options do we have for high-performance liquid gaskets these days?
Read More
Ask Dr. Dave

Can you recommend a safe adhesive for bonding plastics?

With the correct choice of monomers, a UV-cured acrylic will give very strong bonds on these plastics and a crystal-clear bond line.
Dave Dunn, Ph.D.
Dave Dunn Ph.D.
May 2, 2016
Question: We bond interlocking polystyrene and ABS tubes together with a solvent-based cement. Can you recommend a less hazardous and safer adhesive? The plastics are clear.
Read More
Ask Dr. Dave

Have there been any new adhesives for consumer or handyman use recently?

Innovative marketing has given us a couple of very interesting and useful products.
April 1, 2016

Have there been any new adhesives for consumer or handyman use recently?


Read More
Previous 1 2 3 4 5 6 7 8 9 10 … 17 18 Next
Manage My Account
  • Join Adhesives & Sealants Industry
  • Manage My Preferences
  • Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Industrial robot performing plasma surface treatment on an automotive component
    Sponsored byPlasmatreat North America

    Engineering the Molecular Interface: Atmospheric Plasma Cleaning and Activation for Reliable Bonding

  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

news on internet screen

H.B. Fuller Announces Seven Site Closures

news on internet screen

Ancora Calls for Potential Sale of H.B. Fuller

Photo of a person holding a tablet, reading a new story

H.B. Fuller Rejects Ancora’s Second Offer for Building Adhesive Solutions Business

ASI 2026 Top 20 Adhesives & Sealants List

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Adhesives Technology Handbook   3rd Edition

Adhesives Technology Handbook 3rd Edition

See More Products

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing