Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEWS
    • Latest Headlines
    • ASI News Now
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • NEW PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • From the Editor
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • EVENTS
    • ASI Academy
    • Events Calendar
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • DIRECTORIES
    • Buyers' Guide
    • Equipment Handbook
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Sponsor Insights
    • Classifieds
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
    • CONTACT
  • JOIN!
Home » Authors » Edward M. Petrie

Articles by Edward M. Petrie

Formulating UV-Curing Liquid Pressure-Sensitive Adhesives

Edward M. Petrie
November 1, 2008
This article focuses on the many formulation factors that influence the performance of UV-curing pressure-sensitive adhesives (PSAs).
Read More

Bookbinding Adhesives

Edward M. Petrie
May 1, 2008
Bookbinding demands sophisticated adhesive solutions for a very common product.
Read More
SpecialChem fire retardant adhesives

Fire-Retardant Adhesives

This article examines the external events that have led to greater awareness of adhesives’ performance in the event of a fire, the standards and regulations that are being imposed, and the development of new fire-resistant materials.
Edward M. Petrie
November 1, 2007
Historically, fire resistance has not generally been a significant requirement when specifying adhesive systems. Recent incidents, however, indicate that this may soon change. These include events outside of the formulators’ arena, such as increased sensitivity to the performance of components in a fire, and events within the formulators’ arena, such as the development of flame-resistant additives.
Read More
biodegradable polymers

Biodegradable Polymers in Adhesive Systems

Many biodegradable polymers are suited for adhesive applications, such as environmentally friendly packaging, recyclable envelope adhesives and biomedical devices.
Edward M. Petrie
June 1, 2007

Significant advances have been made over the past 20 years in the development of biodegradable polymers. These materials have been developed in a variety of forms, and thus have potential use in a range of industries, including adhesives.


Read More
handwashing

Safety First: Safe Handling of Adhesives and Sealants

While cured adhesives and sealants are generally considered safe, care must be taken with airborne particles, decomposition products, and uncured components.
Edward M. Petrie
March 1, 2007

Completely cured adhesives and sealants are generally considered safe and non-toxic, although caution must be exercised when machining or grinding joints due to airborne particles. Also, decomposition products may exhibit substantial vapor pressures that present health and safety issues. However, it is exposure to uncured components that can be the most harmful, and that is the subject of this article.


Read More
SpecialChem bathtub sealants

How Sealants Function

How do the application and performance characteristics of sealants correlate to the composition of the sealant formulation?
Edward M. Petrie
February 27, 2006
Sealants are generally chosen for their ability to fill gaps, resist relative movement of the substrates, and exclude or contain another material. Sealants are generally lower in strength than adhesives, but have better flexibility. Usually, a sealant must effectively bond to a substrate in order to perform these functions.
Read More
Manage My Account
  • Join Adhesives & Sealants Industry
  • Manage My Preferences
  • Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Industrial robot performing plasma surface treatment on an automotive component
    Sponsored byPlasmatreat North America

    Engineering the Molecular Interface: Atmospheric Plasma Cleaning and Activation for Reliable Bonding

  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

news on internet screen

H.B. Fuller Announces Seven Site Closures

news on internet screen

Ancora Calls for Potential Sale of H.B. Fuller

Photo of a person holding a tablet, reading a new story

H.B. Fuller Rejects Ancora’s Second Offer for Building Adhesive Solutions Business

ASI 2026 Top 20 Adhesives & Sealants List

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Adhesives Technology Handbook   3rd Edition

Adhesives Technology Handbook 3rd Edition

See More Products

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing