AU-1 Commercial Construction Sealant exceeds ASTM C920 Class 35, accommodating 70% total joint movement. It bonds to a broad range of common construction materials without priming on most substrates and seals joints up to two inches wide with proper joint design.
With no petroleum-derived raw materials, AU-1 from Tower Sealants utilizes a water-based, high-performance acrylic urethane polymer. This formulation can help reduce reliance on some of the raw materials and chemistries that have experienced significant cost volatility.
Its paintability, weathering resistance and water-based cleanup make AU-1 a practical choice for demanding residential and commercial applications, including window and door perimeters, siding, masonry and expansion joints.
Visit towersealants.com for more information.