Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEWS
    • Latest Headlines
    • ASI News Now
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • NEW PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • From the Editor
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • EVENTS
    • ASI Academy
    • Events Calendar
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • DIRECTORIES
    • Buyers' Guide
    • Equipment Handbook
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Sponsor Insights
    • Classifieds
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
    • CONTACT
  • JOIN!
Home » industrial coatings

Articles Tagged with ''industrial coatings''

Top 5 News that Sticks

Arkema Acquisition of Ashland Performance Adhesives Garners Most Reader Interest

Readers last week were most drawn to yet another major industry acquisition.
Susan Sutton
Susan Sutton
September 7, 2021

Are you up to date on all of the latest industry acquisitions? Subscribe to the weekly ASI eNews, and we’ll deliver all of the news directly to you!


Read More
Covestro and Hesse

Covestro and Hesse Produce Life Cycle Assessment of Wood and Furniture Coatings

According to Covestro, formulations with Bayhydur quix 306-70 dry as quickly as those with solvent-based crosslinkers, in contrast to coatings with low-VOC, water-based standard hardeners.
August 31, 2021
A study conducted by Covestro and coatings manufacturer Hesse GmbH & Co. KG focused on analyzing the life cycle assessment of different polyurethane wood coatings from raw material production to the applied coating in order to demonstrate the environmental impact of these systems and to reveal advantages and disadvantages for each technology.
Read More

Sika to Divest European Industrial Coatings Business

The product range encompasses anticorrosive and fire protection coatings that are mainly sold in Germany, Switzerland, Poland, and Austria.
August 26, 2021
Sika recently announced that it has agreed to sell its Germany-based European industrial coatings business to The Sherwin-Williams Co.
Read More
acquisitions_mergers_gears

PPG to Acquire Global Coatings Manufacturer Wörwag

Wörwag operates locations in Germany, the United States, China, South Africa, Mexico, Spain, Switzerland, and Poland.
January 26, 2021
PPG recently announced that it has reached a definitive agreement to acquire Wörwag, a global manufacturer of coatings for industrial and automotive applications.
Read More

Environmental Concerns Expected to Help Promote Growth in Global Paints and Coatings Market

Strict environmental regulations, coupled with rising awareness regarding eco-friendly coatings and better alternatives to traditional products, are expected to propel market growth.
December 16, 2020
The global paints and coatings market was estimated to be valued at more than $140 billion in terms of revenue in 2019 and is predicted to grow at a CAGR of 5.4% from 2020-2027.
Read More
ChemQuest coatings study

THE CHEMQUEST GROUP, INC.: Paint and Coatings Industry Market Analyses

These two studies reportedly incorporate findings from in-depth interviews with key industry experts to provide a solid base for analyzing the impact of trends and drivers in major market segments.
July 1, 2020
The ChemQuest Group recently announced the publication and availability of the “U.S. Market Analysis for the Paint & Coatings Industry (2019-2024)” and “Global Market Analysis for the Paint & Coatings Industry (2019-2024).”
Read More

Annual Growth Projected at 4% for Industrial Coatings Market Beginning Next Year

Due to the economic effects of the coronavirus, little to no growth is currently expected for this year; some end uses are declining significantly.
June 8, 2020
Global consumption of paint and coatings was 44.4 million tons (98 billion pounds) in 2019, worth $132 billion.
Read More
Evonik synthetic silica additive

EVONIK: Synthetic Silica for Coatings Formulations

Evonik reports that variations in the wet reaction process conditions enable the control of many aspects of final coatings formulations, such as pH, surface area, pore volume, and other structural or morphological effects.
June 2, 2020
The Coating Additives business line of Evonik recently introduced SPHERILEX silica wet chemistry technology, with three new products.
Read More
Awards

Two PPG Facilities in Ohio Receive Recognition for Environmental, Health, and Safety Initiatives

PPG's Barberton location was presented with an Award for Excellence in Health and Safety Performance, while the Huron facility received recognition for Environmental Performance.
May 13, 2020
PPG recently announced that its Barberton and Huron, Ohio, facilities were recognized by the Ohio Chemistry Technology Council (OCTC) for programs that advance the company’s health, safety, and environmental performance.
Read More
Panacol UV curable coating

PANACOL: Autoclavable UV Coating

Panacol reports that the coating surface is very dry after UV curing, so coated components can be processed immediately.
May 7, 2020
Vitralit 2028 from Panacol is a UV-curable coating that is resistant to chemicals and is autoclavable.
Read More
Previous 1 2 3 4 5 6 Next
Manage My Account
  • Join Adhesives & Sealants Industry
  • Manage My Preferences
  • Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Industrial robot performing plasma surface treatment on an automotive component
    Sponsored byPlasmatreat North America

    Engineering the Molecular Interface: Atmospheric Plasma Cleaning and Activation for Reliable Bonding

  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

news on internet screen

Ancora Calls for Potential Sale of H.B. Fuller

Photo of a person holding a tablet, reading a new story

H.B. Fuller Rejects Ancora’s Second Offer for Building Adhesive Solutions Business

Image of scrabble pieces with pictures of people

Sika Acquires UAE Waterproofing Firm Duproof

ASI 2026 Top 20 Adhesives & Sealants List

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Adhesives Technology Handbook   3rd Edition

Adhesives Technology Handbook 3rd Edition

See More Products

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing