Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEW PRODUCTS
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • EVENTS
    • ASI Academy
    • Events Calendar
  • COLUMNS
    • European Perspectives
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Classifieds
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
      • Custom Content & Marketing Services
    • CONTACT
  • SIGN UP!
Home » Topics » Adhesives and Sealants Topics » Raw Materials and Chemicals

Raw Materials and Chemicals
Raw Materials and Chemicals RSS Feed RSS

news generic
Top 5 News that Sticks

World Adhesive and Sealant Conference Postponement Leads the News

Readers last week were most interested in the coronavirus-related postponement of the World Adhesive and Sealant Conference.
Susan Sutton
Susan Sutton
March 23, 2020

What impact is COVID-19 having on your business? Please contact me at suttons@bnpmedia.com to share your story.


Read More
asi0320-AA-Kaneka-img
Advancing Adhesives

A New Route to High-Performance Flexible Adhesives and Coatings: 2K STPE/Epoxy Technology

Combining a silyl-terminated polyether with epoxy technology as a two-component system provides a balance of high-strength performance and flexibility with bonding properties similar to traditional epoxies.
Ruolei Wang
Ruolei Wang
March 23, 2020
In the past half-century, the global market for sealants and adhesives in construction and industrial applications has experienced significant growth.
Read More

Ashland Announces Price Increases for 1-4 Butanediol and Derivatives in the Americas and Europe

The increases are effective April 1, 2020, or as agreements allow.
March 23, 2020
Ashland recently announced that it is increasing prices on 1-4-butanediol (BDO) and several derivative products.
Read More

Cambrian Solutions Named Distributor for Ingevity Rosin Ester Product Lines in Canada

Ingevity’s bio-based tackifier products reportedly have broad compatibility with multiple polymers commonly used in rigid packaging, hygiene, tapes, labels, and construction adhesives.
March 19, 2020
Ingevity recently announced the appointment of Cambrian Solutions, a Maroon Group company, as distributor for its WestRez and Altatac rosin ester product lines in Canada.
Read More
market trends-2

ExxonMobil Evaluating Significant Near-Term Capital and Operating Expense Reductions Due to COVID-19

The company is closely monitoring the COVID-19 pandemic and has adjusted work arrangements to ensure a healthy work environment and support communities where it operates.
March 19, 2020
ExxonMobil is looking to significantly reduce spending as a result of market conditions caused by the COVID-19 pandemic and commodity price decreases.
Read More
generic chemicals

Huntsman Expands Specialty Chemicals Portfolio with Acquisition of CVC Thermoset Specialties

Under terms of the agreement, Huntsman will pay $300 million, subject to customary closing adjustments, in an all-cash transaction funded from available liquidity.
March 17, 2020
Huntsman Corp. recently announced that it has reached an agreement to acquire CVC Thermoset Specialties, which is part of Emerald Performance Materials LLC.
Read More
chart

Specialty Adhesion Applications Spur Demand for Silyl-Modified Polymers

With silyl-modified polymers offering features of both polyurethane and silicon, the market is receiving immense traction.
March 16, 2020

The silyl-modified polymers market is poised to grow at a CAGR of around 4.6% from 2019-2029, as demand for new and lightweight assembly materials in transportation and wind energy applications soars.


Read More
Ask Dr. Dave

What can I use as an adhesion promoter to a ceramic surface?

Dr. Dave discusses promoting adhesion on ceramic surfaces, as well as curing considerations for anaerobic adhesives.
Dave Dunn, Ph.D.
Dave Dunn Ph.D.
March 16, 2020
In general, a ceramic surface tends to behave similarly to a glass surface.
Read More
news generic

World Adhesive and Sealant Conference Postponed

ASC reports that it is working to secure dates to reschedule WAC2020 at the same venue for a later date in 2020.
March 13, 2020

The Adhesive and Sealant Council (ASC), organizer of the World Adhesive and Sealant Conference, has announced that the event will be postponed due to COVID-19.


Read More

Azelis Americas CASE Appointed U.S. Distributor for Momentive Polyurethane Additives

Effective May 10, 2020, the agreement expands Azelis’ commercial relationship with Momentive.
March 13, 2020

Azelis Americas CASE, LLC recently announced that it has been appointed U.S. distributor by Momentive Performance Materials USA LLC for its polyurethane additives products.


Read More
Previous 1 2 … 177 178 179 180 181 182 183 184 185 … 390 391 Next
Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

image of handshake

APPLIED Adhesives Expands Silicone Solutions and East Coast Presence with Acquisition

People shaking hands

Henkel Names Exclusive US Distributor for Flexible Packaging Technologies

Picture of a lobby of a Henkel facility

Henkel Expands Silicon Valley Application Center for Electronics

ASI 2026 Top 20 Adhesives & Sealants List

Events

September 15, 2026

Coatings Trends & Technologies Summit

This annual Midwest coatings conference combines all of the high-quality technical presentations, exhibits and networking opportunities from the Coatings Trends and Technologies and Powder Coating Summit conferences into one new event. The event caters to both liquid and powder coatings formulators and manufacturers.

September 16, 2026

World Adhesive & Sealant Conference (WAC) 2026

As the industry’s premier international event, WAC 2026 offers a unique opportunity for professionals from every continent to connect, collaborate, and shape the future of the sector.
View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing