EpoxySet to Feature Award-Nominated, Delay-Cure Adhesive at MD&M WEST
The one-part epoxy can reportedly be activated by UV or blue light from 365-405 nm with an intensity of about 150 mW/cm2 for 5-10 sec.

EpoxySet Inc. recently announced that it will showcase its FLASHBOND™ UV-5608DC delay-cure epoxy at MD&M West, which will be held February 11-13, 2020, in Anaheim, Calif. According to the company, FLASHBOND UV-5608DC allows for fast processing and fixturing of parts, even if both parts are opaque.
The one-part epoxy can reportedly be activated by UV or blue light from 365-405 nm with an intensity of about 150 mW/cm2 for 5-10 sec. Parts are then mated together and aligned within 45-60 sec of activation. The adhesive yields green strength after 30 min for handling. Full cure occurs over the next 16 hrs at room temperature.
For more information, visit www.epoxyset.com. Details regarding MD&M West are available at https://mdmwest.mddionline.com.