Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEWS
    • Latest Headlines
    • ASI News Now
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • NEW PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • From the Editor
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • EVENTS
    • ASI Academy
    • Events Calendar
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • DIRECTORIES
    • Buyers' Guide
    • Equipment Handbook
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Sponsor Insights
    • Classifieds
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
    • CONTACT
  • JOIN!
Home » Topics » News » Adhesives & Sealants Headlines

Adhesives & Sealants Headlines
Adhesives & Sealants Headlines RSS Feed RSS

Univar Solutions to Distribute Dow Polyurethanes in North America

Univar Solutions will serve as an authorized channel for Dow’s polyurethane products across the U.S. and Canada.
June 7, 2019
Dow and Univar Inc. recently announced that Dow has selected Univar Solutions as a key North American channel to market, distributing Dow’s product portfolio of polyols and isocyanates.
Read More
Raised-Hands

Ford’s Mikula to Keynote 2019 ASSEMBLY Show

During his keynote presentation, Mikula will discuss how Ford is using state-of-the-art production tools and processes to make the vehicles of tomorrow.
June 7, 2019
Michael Mikula, chief engineer for Advanced Manufacturing at Ford Motor Co., will give the keynote address at The ASSEMBLY Show, which will be held October 22-24 in Rosemont, Ill.
Read More
Awards

Huntsman Polyurethanes Names Maroon Group Distributor of the Year

The award was presented to Maroon Group’s sales and operations staff in appreciation for Sales Growth and New Business Development.
June 6, 2019
Huntsman Corp.’s Polyurethanes Division has recognized Maroon Group as its 2018 Distributor of the Year.
Read More

Sika Opens Concrete Admixtures Production Facility in Qatar

In addition to production lines for concrete admixture manufacturing, the main office and a central storage facility will be located at the site.
June 6, 2019
Sika recently announced that it is starting operations at a plant in Doha, Qatar, for the production of concrete admixtures.
Read More
Henkel Governor Murphy

Henkel Showcases Sustainable Solutions for New Jersey Governor Phil Murphy

Henkel shared several solutions that the adhesives technical teams are developing to enable and enhance sustainable and recyclable products in the packaging, consumer, and constructions industries.
June 5, 2019
Henkel Corp. recently welcomed Governor Phil Murphy to its facility in Bridgewater, N.J., to showcase products and designs for customers to enable more sustainable and environmentally friendly solutions for consumers.
Read More

Covestro Supports 2019 Carbon Footprint Challenge

The Carbon Footprint Challenge invites students and young professionals from all over the world to share ideas to fight climate change on an open innovation online platform.
June 5, 2019
Covestro recently announced that, for the second consecutive year, it is a partner of the global Carbon Footprint Challenge, an international business idea competition supported by leading global companies such as Bühler, Evonik, and Oracle, as well as nine top European universities connected to the Unitech network.
Read More
ViscoTec Innovation Days

Innovation Days at ViscoTec Focus on Transfer of Cross-Industry Knowledge

How should dispensers, dosing, and filling pumps be designed in order to apply liquids with one or more components?
June 4, 2019
Almost 400 experts from 32 nations recently met at ViscoTec’s Customer & Innovation Days (CID).
Read More
Synthomer EDANA

Synthomer Joins International Association Representing the Nonwovens and Related Industries

Along with EDANA’s 250 members, Synthomer aims to advance the interests of the nonwovens and their related industries in working groups, industry expositions, and events.
June 4, 2019
Synthomer recently announced that it has joined the International Association Representing the Nonwovens and Related Industries (EDANA) as an official member.
Read More
Bostik PSTC poster

Bostik Wins Innovative Poster Session at PTSC Tape Summit

Christophe Robert, Bostik EMEA’s PSA manager, presented on moisture-cured pressure sensitive adhesive (PSA) technology and earned the award.
June 3, 2019
Bostik recently announced that it was the recipient of the Best Poster Award during the Innovative Poster Session at the Pressure Sensitive Tape Council’s (PSTC) recent Tape Summit in Baltimore, Md.
Read More
CMC Milling Dave Morse

Morse of DRM Chemical Process Services to Consult for CMC

Bringing more than 37 years of experience in the chemical processing and specialty inks industries, Morse will offer his services as a process consultant for a wide range of industries.
June 3, 2019
Custom Milling & Consulting, Inc. (CMC) recently announced its new association with DRM Chemical Process Services, which is owned and operated by Dave Morse.
Read More
Previous 1 2 … 384 385 386 387 388 389 390 391 392 … 1028 1029 Next
Manage My Account
  • Join Adhesives & Sealants Industry
  • Manage My Preferences
  • Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Industrial robot performing plasma surface treatment on an automotive component
    Sponsored byPlasmatreat North America

    Engineering the Molecular Interface: Atmospheric Plasma Cleaning and Activation for Reliable Bonding

  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

news on internet screen

Ancora Calls for Potential Sale of H.B. Fuller

Photo of a person holding a tablet, reading a new story

H.B. Fuller Rejects Ancora’s Second Offer for Building Adhesive Solutions Business

image of a graph representing markets

H.B. Fuller Announces Debt Offering to Help Fund AMS Acquisition

ASI 2026 Top 20 Adhesives & Sealants List

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Adhesives Technology Handbook   3rd Edition

Adhesives Technology Handbook 3rd Edition

See More Products

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing