Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEW PRODUCTS
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • EVENTS
    • ASI Academy
    • Events Calendar
  • COLUMNS
    • European Perspectives
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Classifieds
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
      • Custom Content & Marketing Services
    • CONTACT
  • SIGN UP!
Home » Topics » News » Adhesives & Sealants Headlines

Adhesives & Sealants Headlines
Adhesives & Sealants Headlines RSS Feed RSS

handshake

R.E. Carroll Launches Brand Promise to Industry

The promise includes “Knowledgeable, Responsible, Trusted: What Matters To You Is Important To Us.”
July 12, 2019
R.E. Carroll Inc. recently announced that it has launched a new “Brand Promise to the Adhesives Industry.”
Read More
Nordson Sundaram Nagarajan

Nagarajan Named President and CEO of Nordson

Sundaram Nagarajan joins Nordson following a 23-year career with Illinois Tool Works Inc. (ITW), serving most recently as executive vice president of the $3.3 billion Automotive OEM segment.
July 11, 2019
Nordson Corp. recently announced that Sundaram Nagarajan (Naga) has been appointed president and CEO, effective August 1, 2019.
Read More
Headlines 3

Gelest Acquires Bimax

Bimax will continue to operate under the Bimax name, and all employees will be retained in their current roles.
July 11, 2019

Gelest, Inc. recently announced its acquisition of Bimax, a manufacturer and marketer of specialty monomers and polymers for use in the manufacture of contact lenses, intraocular lenses, personal care products, coatings and adhesives, and other advanced technology applications.


Read More
acquisitions_mergers_puzzle

Synthomer Announces Agreement to Acquire OMNOVA Solutions

OMNOVA Solutions employs approximately 1,900 people and operates 13 sites across the U.S., Europe, and Asia.
July 10, 2019
Synthomer plc recently announced that it has reached an agreement with OMNOVA Solutions Inc. on the terms of a recommended acquisition of the entire issued and to-be-issued share capital of OMNOVA.
Read More
shopping_cart

Brenntag Expands U.S. Lubricants Business with Acquisition of B&M Oil

B&M Oil generated sales of $28.5 million in 2018.
July 10, 2019
Brenntag recently announced its acquisition of B&M Oil Co., a regional lubricants distributor headquartered in Tulsa, Okla.
Read More
Generic_News

U.S. Chemical Industry Expansion Continues Despite Headwinds

Chemical industry growth is projected to exceed that of the U.S. economy through 2024.
July 10, 2019
U.S. chemical industry output will continue to grow in 2019 despite a challenging global economy, according to the American Chemistry Council.
Read More

LANXESS Launches High-Performance Prepolymers Production in Brazil

In addition to increasing production capacity, the company reports that application development and technical services are provided from a state-of-the-art laboratory at the site.
July 9, 2019
LANXESS recently announced that it has started the production of high-performance prepolymers at its site in Porto Feliz, Brazil.
Read More
FEICA Currenta isocyanate standard

FEICA Signs Off on Validation Report for Isocyanate Test Method

FEICA reports that the validated test method is able to measure isocyanates down to a range of 0.01-0.15%.
July 9, 2019
FEICA recently announced that it has signed off on the Validation Report of the Currenta test method for the accurate measurement of low contents of free monomeric isocyanate in mixtures.
Read More
headlines and news

ALTANA Acquires Paul N. Gardner

Within the ALTANA Group, the business will be integrated into the Instruments Business Line of the BYK Division (BYK-Gardner).
July 8, 2019
ALTANA recently announced that it has acquired the operating assets of the Paul N. Gardner Co. Inc. (GARDCO) of Pompano Beach, Fla.
Read More
acquisitions_mergers1

Berry Global Announces New Business Structure and Leadership Appointments

Berry’s business structure will now be comprised of four divisions: Consumer Packaging–International; Consumer Packaging–North America; Engineered Materials; and Health, Hygiene, and Specialties.
July 8, 2019
Berry Global Group, Inc. recently announced a new business structure linked to the company’s recent acquisition of plastics and plastic packaging manufacturer RPC Group Plc.
Read More
Previous 1 2 … 356 357 358 359 360 361 362 363 364 … 1004 1005 Next
Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

Photo of shoe on shovel breaking into dirt

H.B. Fuller to Open Aerospace Manufacturing Center of Excellence

Image of a blue bar chart with arrow pointing up

Iran War and Logistics Challenges Impact Adhesives and Sealants Pricing

news on internet screen

H.B. Fuller and Ancora Holdings Clash Over Proposed Medical Adhesives Acquisition

ASI Top 20 website

Events

June 15, 2026

Adhesive and Sealant Council Executive Leadership Conference

This annual event provides current and future leaders in the adhesives and sealants industry with the opportunity to expand their knowledge and network with peers.

September 14, 2026

Women in Chemicals Conference

Organized by Women in Chemicals, this landmark conference will offer opportunities for networking, learning, and professional development. With a diverse array of sessions, workshops, and social events, participants can expect a dynamic program designed to empower and inspire.

View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

ASI CASE EBOOK

ASI raw materials roundup

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing