Inspired by nature, a newly developed adhesive to help restore reefs is biocompatible and biodegradable, attributes essential for use in this extremely delicate environment.
The growing demand from the packaging industry for lightweight, sustainable, and inventive packaging options is anticipated to boost the bio-based adhesives market.
Mussels' unique and remarkable ability to stick to underwater surfaces has inspired a new, more efficient, and environmentally friendly way to extract critical rare earth elements.
A two-component, ultra-low density, flame-retardant polyurethane foam is designed for potting and encapsulating lithium-ion battery cells in EV battery modules.
An innovative foam encapsulant is designed to protect the vehicle, the passengers, and the EV industry from the dangers of battery fires.
A de-inkable, recyclable, mono-material polyethylene pouch received the award for Recyclability/design for Recycling, representing the value of partnerships along the value chain.