Encor®182 latex can be used to meet ASTM C 834/0°C specifications or blend it with acrylic binders to meet ASTM C 834/-17°C specifications, if required.
The range includes a universal surface-insensitive cyanoacrylate of medium viscosity that can reportedly bond many substrates in seconds; a fast-curing plastic and rubber cyanoacrylate of low viscosity; and a cyanoacrylate non-drip gel that reportedly stays in place when dispensed.
A new range of cyanoacrylate and anaerobic adhesives is now available.
Loctite®SI 5640™ is a new two-part, self-leveling silicone potting compound designed for electrical and electronic potting applications that require UL 94 VO compliance.