Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEWS
    • Latest Headlines
    • ASI News Now
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • NEW PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • From the Editor
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • EVENTS
    • ASI Academy
    • Events Calendar
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • DIRECTORIES
    • Buyers' Guide
    • Equipment Handbook
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Sponsor Insights
    • Classifieds
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
    • CONTACT
  • JOIN!
Home » Topics » Adhesives & Sealants Industry Top Stories

Adhesives & Sealants Industry Top Stories
Adhesives & Sealants Industry Top Stories RSS Feed RSS

scientists discussing

Formulating with Flexibility

Finding solutions to meet ever-evolving demands encourages flexibility and collaboration with suppliers, formulators and customers.
Edwin Hortelano Ph.D.
October 30, 2023

More than any single piece of lab equipment, a successful R&D team’s most vital tool is a flexibility mindset.


Read More
electric vehicle charging

Adhesive Solutions for e-Mobility Applications

Adhesive tape offers a variety of solutions in the design and manufacturing of electric vehicles, including insulation, mounting and bonding, and thermal interfaces.
Daniel Heini
October 27, 2023

As demand for electric vehicles (EVs) grows, adhesive tapes continue to play an important role in the engineering and manufacturing of EVs.


Read More
chemistry in motion

New Acrylic Block Elastomer for Adhesive Applications

Developed using proprietary living anionic polymerization technology, a new acrylic thermoplastic elastomer is suitable as an adhesive for masking tape, packaging, surface protection film, double-sided tape, and as an anti-slip film.
Erich Klein
October 25, 2023

A new acrylic TPE is suitable as an adhesive for masking tape, packaging, surface protection film, double-sided tape, as an anti-slip film, and it has a wide range of applications beyond adhesives.


Read More
polymerresearch.jpg

AI Algorithm Is Accelerating Polymer Research

A new tool developed by scientists at Georgia Tech captures patterns and relationships and learns the grammar and syntax that occur at the atomic and higher levels in polymer structures.
October 24, 2023

PolyBERT treats chemical structures and connectivity of atoms as a form of chemical language and uses techniques inspired by natural language processing to extract the most meaningful information from chemical structures.


Read More
colors mixing

Influence of Rheology on Mixing Behavior in Static Mixers

The second of a series on static mixing, this article focuses on how the rheology of a material impacts mixing behavior.
Joachim Schöck
October 20, 2023

When selecting the optimum static mixer, the rheological properties of the starting components and their mixing ratio play an important role.


Read More
painting building exterior with areas protected by protective adhesives

Adhesive and Sealant Technologies for Masking Tapes Solve the Painting Industry’s Peskiest Problems

As new paint technology comes on the market, manufacturers of painter’s tapes are developing more targeted adhesives and sealants that create clean lines while solving issues associated with masking rough or difficult-to-stick-to surfaces.
Patti LaPorte
October 16, 2023

With options like exterior painter’s tape that works on self-cleaning paint and sealant technology that works with paint chemistry to prevent paint bleed, painters now have more specialized tape options to produce professional results under virtually any condition.


Read More
GettyImages-1469964188-static.jpg

Reactive Polyamide Oligomers for Elastomeric, Adhesive, and Coating Applications

Improvements made to the processability of polyamide oligomers resulted in the discovery of a novel soft segment chemistry that is viable not just for waterborne coating application but for elastomers, adhesives, and possibly other urethane applications
Gabor Erdodi Alec Krienen Chandra Pandey Romina Marin
October 13, 2023

Polyurethanes with tertiary polyamide segments have excellent abrasion resistance coupled with high hardness, good hydrolytic stability, improved barrier properties and strong adhesion to various polar substrates.


Read More
GettyImages-1442852776.jpg

Assemble, Automate, and Accelerate at the 2023 ASSEMBLY Show

The ASSEMBLY Show promises engineers and manufacturing executives an in-depth look at the latest innovation in assembly technology.
karen parker
Karen Parker
October 13, 2023

The 11th annual ASSEMBLY Show will take place from October 24-26, 2023 at the Donald E. Stephens Convention Center in Rosemont, Illinois.


Read More
GettyImages-1174552855.jpg

Industry Leaders to Discuss a Sustainable Future at ASC Executive Leadership Conference

With the theme, “Building a Sustainable Future,” the conference will focus on key issues facing manufacturers and their suppliers and facilitate informal discussion and networking.
karen parker
Karen Parker
October 10, 2023

Executives in the adhesives and sealants industry will gather at the Ponte Vedra Inn & Club in Ponte Vedra Beach, Florida, October 23-25 for the Adhesive and Sealant Council’s Executive Leadership Conference.


Read More
GettyImages-898393796-static.jpg

The Latest Market and Technology Trends in Solvent-free Lamination Adhesives

Enhanced polyurethane solvent-free laminating adhesive systems facilitate the replacement of solvent-based adhesives, while addressing critical challenges of increasing usability.
October 6, 2023

Toyo-Morton estimates that CO2 emissions related to inks and laminating adhesives in packaging can be reduced up to 70% by substituting solvent-based products with solvent-free ones.


Read More
Previous 1 2 … 27 28 29 30 31 32 33 34 35 … 120 121 Next
Manage My Account
  • Join Adhesives & Sealants Industry
  • Manage My Preferences
  • Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Industrial robot performing plasma surface treatment on an automotive component
    Sponsored byPlasmatreat North America

    Engineering the Molecular Interface: Atmospheric Plasma Cleaning and Activation for Reliable Bonding

  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

news on internet screen

H.B. Fuller Announces Seven Site Closures

image of a graph representing markets

Arkema Reports 8.1% Sales Growth in Third Quarter

Picture of men and women standing at a ribbon cutting

Henkel Opens New Adhesives Application Center in Indonesia

ASI 2026 Top 20 Adhesives & Sealants List

Events

April 3, 2027

APEX Expo 2027

Explore the latest technologies, materials, and innovations in electronics manufacturing at APEX Expo 2027, April 3–8 in Anaheim, California, with educational sessions and industry networking opportunities.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Adhesives Technology Handbook   3rd Edition

Adhesives Technology Handbook 3rd Edition

See More Products

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing