the credit crunch pushes blade demand below supply levels, getting a durable
product made reliably and efficiently has never been more important. Adhesive
can play a key role in this goal.
Innovation-based startup company Lumina Adhesives has developed a new technology platform of switchable pressure-sensitive adhesives called AdhelightTM that enables debonding on demand.
Pressure-sensitive adhesives (PSAs) are used in applications ranging from labeling food packaging to assembling electronic devices to mounting graphics displays. Although they have been around for decades and their use is widespread, manufacturers, converters, and printers may not understand the key differences between the adhesive choices available, how they’re constructed, or which are best suited for a particular job.
Researchers at the University of Chicago and Lawrence Berkeley National Laboratory have developed an “electronic glue” that could accelerate advances in semiconductor-based technologies, including solar cells and thermoelectric devices that convert sunlight and waste heat, respectively, into useful electrical energy.