This company introduces optiFLEX(r) CONFORM(tm) (PP25011, PP25012, PP25021 and PP25022) flexible films that offer excellent conformability, affordability and quick-ship availability. These 2.5-mil, conformable polypropylene films have been designed for labeling semi-squeeze and rigid containers with irregular shapes and compound curves. Applications include beverage, household/chemical and personal care. Circle No. 117